PPG Earns Recognition for Anionic Epoxy Electrocoat
PITTSBURGH — PPG announced that its PPG POWERCRON® 160 anionic epoxy electrocoat (e-coat) technology has earned a 2019 R&D® 100 Award in the Mechanical/Materials category.
“Earning an R&D 100 Award is a pinnacle of achievement in the global research and development community, and we are proud to be recognized for this groundbreaking coatings technology,” said David Bem, PPG Vice President, Science and Technology, and Chief Technology Officer. “We are even prouder of what this development means for our customers – more versatile and effective corrosion protection for their products with less energy use and enhanced environmental compliance.”