Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Industrial Coatings

Antiviral Coatings in Covid Times

By Grand Polycoats
Antiviral Coatings in Covid Times
source: Getty Images
August 5, 2021

Can you recollect the number of times you furiously wiped surfaces with disinfectants over the past year? The COVID-19 fear factor has demanded scientists research products that are based around nanotechnology. They have been looking for several options that aim at surface coatings that tend to bond with materials and provide them with long-term protection against viruses, bacteria and fungi.

 

Why Do You Need An Antiviral Coating?

Hygienic or antimicrobial coatings have been around for the past several years. Apart from using preservatives just for in-can preservation, these coatings offer active protection against several microorganisms like bacteria, fungi, viruses, etc. when applied in the film state. They have a wide range of applications that include air conditioning and heating systems, medical implants, food processing facilities and equipment, home appliances, ship hulls, and personal care. These coatings are extremely useful to us today in the light of the pandemic since they are also used as coatings for floors, walls, institutional and industrial countertops, railings of schools, hospitals, and are also sprayed onto gloves, masks and textiles. Both powder and liquid forms are available today for coating purposes on these surfaces to prevent the spreading of several diseases.

A virus such as SARS-CoV-2, the one that caused the global COVID-19 pandemic, typically ranges in size from 100 to 300 nm and is smaller in size when compared to bacteria. It comprises DNA or RNA surrounded by proteins that offer them protection from the environment and help them to bind to specific sites in the host cells. These kinds of enveloped viruses also have an outer layer made from proteins, lipids and polysaccharides that enable the viruses to more easily combine and enter the host cells. For surviving and reproducing they must infect a living host cell. However, coronaviruses like SARS-CoV-2 have been proved to survive on glass, metal, wood, plastic and fabric surfaces for many hours to days. Hence, destroying or damaging them in their existence on surfaces can help in preventing infection and the spread of diseases.

Several different kinds of nanoparticles such as nanoscale spurious oxide, silver, zinc oxide, quaternary ammonium cations, and gold on silica have proven to be effective to inactivate viruses, including SARS-CoV-2.

 

What are Antiviral Coatings?

Much research has been focusing on developing antiviral coatings due to the COVID-19 pandemic. Antiviral coatings are known to be a subset of antimicrobial coatings. Some of these antimicrobial coatings possess the capability to kill viruses, bacteria and other microorganisms like fungi and mold, whereas others do not destroy viruses.

One such example of a coating approved by the U.S Environmental Protection Agency that tends to target viruses is the Caliwel BNA Coating by Allistagen Corporation. This coating features calcium hydroxide and is proven to be effective against 20-plus life-threatening viruses, bacteria and fungi.

Several researchers at the Hong Kong University of Science and Technology have reported that the development of an antiviral coating could offer 90 days of protection against viruses and bacteria, including SARS-CoV-2, when it is sprayed onto frequently touched surfaces.

This coating is based on multilevel antimicrobial polymer or MAP-1. It consists of millions of nano capsules that are formed with heat-sensitive polymers containing disinfectants. These polymers release the disinfectants when they are warmed by human hands.

Speaking of development, 1X ViroCoat of Grand Polycoats, was recently launched in the Indian market. This anti-viral coating contains silicon polymer and active nano additives that safeguard against viruses for up to 90 days. It is made with a special resin that has the quality to adhere to multiple surfaces such as metal, plastic, wood, glass, ceramic, etc. 1X ViroCoat not only clears out the viruses but also repels it, thereby keeping the sprayed surfaces safe.

It can be summarized that antiviral coating with the active ingredient stays on the surface after application and it is able to neutralize the virus along with other microorganisms such as bacteria, fungi and molds. The presence of active ingredient distinguishes the antiviral coatings as a living polymer coating from the other more general coatings known to the common people.

 

What are Surface Protectors?

Surface protectors are substances that make use of either metal like copper and silver or biomolecules like neem extracts, commonly known for their antimicrobial activity, or positively charged polymers combined with nitrogen compounds like ammonia that are useful in providing a long-lasting protective coating. This compound can be sprayed on glass, metal, stone, wood, leather, fabric, and several other materials. Its effect can last from one week to even 90 days, depending on the kind of surface on which it has been used.

 

Why Can’t Regular Disinfectants be Used?

You can use regular disinfectants, but as they contain either alcohol as in sanitizers, or active chlorine as in sodium hypochlorite or other halogen combinations, the active ingredients in such solutions dissociates or evaporates from the surface very fast. This limits the activity of the active ingredient, hence making it ineffective over longer durations of time. These chemicals are hazardous in nature, and can cause great damage to the environment with its prolonged usage.

 

Acknowledgment

The author would like to express gratitude and regards to Mr. Ankur Chokshi and management of Grand Polycoats for contributing to the generation of data and helping us in conducting the tests and experiments smoothly. Grand Polycoats is amongst the most reputed and leading manufacturers of industrial coatings and paints. They specialize in providing you with high-quality and high-performance coatings and paints depending on your needs, catering to several different sectors such as construction, automotive, defense, power and electrical, and process industry.

KEYWORDS: antiviral coatings COVID-19

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

By Grand Polycoats

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett

Post a comment to this article

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

  • colorful building exterior
    Sponsored byDow

    Insights into Exterior Architectural Coating Degradation: Bridging Accelerated and Natural Weathering

Popular Stories

Supply chain question and cargo piles up and piling shipping containers question concept

Energy Disruptions Begin to Hit Coatings Supply Chain

basf

BASF Coatings Names Incoming CEO Ahead of Separation

PPG announced the installation of a state-of-the-art pilot finishing line that features IPG’s PhotoniCURE™ laser curing system at its powder manufacturing and technical facility in Strongsville, Ohio.

PPG Tests Laser Curing for Powder Coatings

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

March 31, 2026

Durability by Design: Waterborne Concrete Coatings that Protect, Beautify, and Extend Service Life

Attend this webinar to understand how protecting concrete enables lifespan extension and reduction of the CO₂ emissions associated with premature repair or replacement.
View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Register for webinar: Next-Gen Dispersion Technology in Paint Production

Related Articles

  • functional materials

    COVID-19 Response: Improved Antiviral Surfaces and Smart Disinfectants

    See More
  • Innovations in Antimicrobial and Antiviral Coatings

    Innovations in Antimicrobial and Antiviral Coatings

    See More
  • Automotive Paints and Coatings Industry in the Battle Against COVID-19

    Automotive Paints and Coatings Industry in the Battle Against COVID-19

    See More

Related Products

See More Products
  • durability.jpg

    Increasing the Durability of Paint and Varnish Coatings in Building Products and Construction 1st Edition

See More Products

Related Directories

  • Stonebridge Coatings Laboratory Inc.

    Stonebridge Coatings Laboratory, Inc., is an independent testing lab serving the paint, coatings, and related industries, offering formulation, product development, testing, problem-solving, competitive benchmarking, failure analysis, reverse engineering, and more. Stonebridge assists in identifying customer needs, developing a plan to address them, implementing the work, and communicating the outcome. Stonebridge is an ISO 17025 Accredited laboratory.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing