Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Company NewsFinishing News

Hempel Launches Its First Leading Edge Protection Coating for Wind Blades

hempelblade
Courtesy of Hempel.

Courtesy of Hempel.

September 21, 2022

Hempel, coatings supplier to the wind energy industry, announced the launch of Hempablade Edge 171, a new coating for leading edge protection (LEP) on wind turbine rotor blades. According to Hempel, Hempablade Edge 171 has the highest rain erosion performance data on the market for a liquid LEP, some of the lowest dry film thicknesses, provides long-term protection against rain erosion, and reduces time and costs during application.

The leading edge of a wind turbine blade is exposed to extremely high airflow speeds, even exceeding 300 kmh. At these speeds, impact from rain can cause significant coating erosion or even composite damage. In severe cases, the erosion may lead to a loss of aerodynamic performance and a 2-3% drop in annual energy production. This loss of performance and need for maintenance makes leading edge erosion one of the wind industry’s most significant maintenance costs and performance challenges. In the European offshore wind energy sector alone, this equates to a loss in productivity of around €56-75 million a year.

Hempablade Edge 171 helps wind turbine operators and applicators overcome these issues by protecting the leading edge from rain erosion, as Lars Rindom Jensen, head of Solutions for Wind Blades, explained, “Hempablade Edge 171 is one of the simplest LEP solutions on the market to apply, yet able to withstand the toughest environmental conditions. It provides exceptional protection against rain erosion and composite damages. This extends the interval between maintenance and repairs, giving operators more uptime and lower maintenance costs.”

Hempablade Edge 171 requires some of the lowest dry film thickness on the market – just 150 microns – and only needs one or two coats to ensure high protection. This increases application speeds, allowing customers to maintain more blades with the resources available.

“Hempablade Edge 171 has been developed as we listened to the industry challenges and requirements,” said Jensen. “Its low thickness reduces LEP consumption, application time and drying time, so applicators can work faster, whether they are onsite or in the blade production. It also has a wide application window – from 5-35 °C – which means applicators can extend the maintenance season and working day. The result is higher productivity and less blade downtime during maintenance.”

Hempablade Edge 171 is Hempel’s first LEP coating, developed using the company’s in-house Rain Erosion Test (RET) facility. Since 2019, Hempel has used this facility to optimize the product development and LEP validation process. With the addition of the coating to its portfolio, Hempel can now provide a full range of coatings for every part of a wind turbine.


For more information, visit: www.hempel.com/blades.

KEYWORDS: Protective Coatings

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

  • colorful building exterior
    Sponsored byDow

    Insights into Exterior Architectural Coating Degradation: Bridging Accelerated and Natural Weathering

Popular Stories

Supply chain question and cargo piles up and piling shipping containers question concept

Energy Disruptions Begin to Hit Coatings Supply Chain

basf

BASF Coatings Names Incoming CEO Ahead of Separation

PPG announced the installation of a state-of-the-art pilot finishing line that features IPG’s PhotoniCURE™ laser curing system at its powder manufacturing and technical facility in Strongsville, Ohio.

PPG Tests Laser Curing for Powder Coatings

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

April 28, 2026

Next Gen Dispersion Technology in Paint Production: Driving Higher Quality at Lower Costs

Join this webinar to see how manufacturers reduce costs, energy use, raw materials, labor, and floor space while improving quality.

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Register for webinar: Next-Gen Dispersion Technology in Paint Production

Related Articles

  • Hempel Launches Leading Intumescent Coating Estimation Software.jpg

    Hempel Launches Leading Intumescent Coating Estimation Software

    See More
  • coatings for wind turbines

    Vestas and Hempel Partner to Develop Surface Protection for Wind Turbines

    See More
  • Image 1.png

    Safeguarding Wind Turbine Blades with Polymeric Technology Supports a Net-Zero Future

    See More

Related Products

See More Products
  • corrosion of linings.jpg

    Corrosion of Linings & Coatings: Cathodic and Inhibitor Protection and Corrosion Monitoring

  • Hansen Solubility Parameters – A Scientific Approach for Coating Formulators (Virtual Course - 8/20/26)

  • intelligent.jpg

    Intelligent Coatings for Corrosion Control 1st Edition

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing