New Powder Primer for High-Performance Corrosion Protection from PPG
PPG announced the launch of the PPG ENVIROCRON® Primeron primer powder portfolio, designed to provide high corrosion resistance for metal substrates including steel, hot-dip-galvanized steel, metalized steel, and aluminum.
The primer powder portfolio has been tested according to the corrosivity categories and approved by the QUALISTEELCOAT international quality label for coated steel. The series covers a wide range of requirements depending on end use, operating environment, and the substrate used: