Research has shown that a thin cellulose film can inactivate the SARS-CoV-2 virus within minutes, inhibit the growth of bacteria including E.coli, and mitigate contact transfer of pathogens.
The coating consists of a thin film of cellulose fiber that is invisible to the naked eye, and is abrasion resistant under dry conditions, making it suitable for use on high-traffic objects such as door handles and handrails.