Ship Owners Save $8 Billion and 41 Million Tonnes of CO<sub>2</sub> with Biocide-Free, Foul-Release Coating
Real-world performance data compiled from ships applied with International® brand Intersleek® 1100SR, over the past 10 years, shows the coating has slashed ship fuel bills by $8 billion and reduced 41 million tonnes of CO2 emissions.
The world-leading biocide-free, foul release coating revolutionized the coatings industry when it was launched by AkzoNobel in 2013, and has been applied to more than 3,000 vessels since then.