Dow Corning Awarded Best Paper at Coatings for Plastics Symposium
A
presentation given by Dow Corning’s Fluorine Technology Program Sales
Development Manager, Steven R. Block, at the 10th Annual International Coatings
for Plastics Symposium was awarded The Best Paper of the Symposium.
Titled, New Chemistry Improves Surface Performance, the presentation was based
on work by Dow Corning and Daikin Industries Ltd. It focused on high-value
fluorosilicone hybrid coatings with notable advantages over current coating
technologies. The new technology will be shown to provide high hardness, high
flexibility, adhesion to low-surface-energy surfaces, chemical resistance, fast
cure at low temperatures and high gloss properties of the coatings.