Thickness Measurement
The new MiniTest FH 7000 Series features SIDSP® (Sensor-Integrated Digital Signal Processing) technology, which provides greater accuracy and repeatability.
Paul N. Gardner Co., Inc.: The new MiniTest FH 7000 Series features SIDSP® (Sensor-Integrated Digital Signal Processing) technology, which provides greater accuracy and repeatability. It offers faster scan rates and the ability to measure down into tighter radius areas. It measures up to 400 mils, allows measurement on non-ferrous materials, and offers SPC capabilities and a menu-controlled user interface.
Visit www.gardco.com.