AkzoNobel’s Interpon has become the first-ever full-body monocoat powder coating to be used on a passenger vehicle in Europe. Showcased at the Cannes SURCAR 2011 Congress, the Citroën DS4 is the first-ever passenger vehicle in Europe to be exhibited using matt black textured powder coatings on the car body.