New Technology Makes Wood-Plastic Composites "Paintable" - Posted 10/10/07
INFIN™ Coating Technology, a new process to coat wood plastic composites in virtually any color while enabling them to resist fading, heat retention, mold, mildew, stains and abrasion, was introduced at the 2007 Wood-Plastics and Natural Fiber Composites Show in Baltimore, MD, October 8 and 9. The technology was jointly developed by Inhance/Fluoro-Seal Ltd. and Finishes Unlimited.