BICESTER, UK – Hardide Coatings, a UK-based provider of advanced tungsten carbide-based coatings, has signed a supply agreement with the General Electric Co. Inc. (GE).
The agreement is for the supply of coating to a single component currently used by GE. It will result in guaranteed turnover volume to the company of approximately $1.3 million over the two years to February 2016. The agreement is extendable up to five years. Development and testing work is also being done on additional components which, if successful, will be included to the agreement, resulting in further minimum annual volumes.