Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Home » Extenders

Articles Tagged with ''Extenders''

OPTI MATT™ MT 8

Acrylic Emulsion Extender Improves Scuff and Mar Resistance in Low-Sheen Coatings

April 21, 2026
No Comments

A 100% acrylic emulsion extender improves scuff and mar resistance while reducing inorganic extender use in low-sheen coating formulations.


Read More
Paint brush and open paint can overlayed with flowers

Zero-Carbon Calcium Carbonate

For paint and coatings
Bill Bryant
December 3, 2025
One Comment

A new calcium carbonate with a negative carbon footprint allows formulators to reduce Scope 3 emissions while maintaining performance.


Read More

KaMin to Buy BASF’s Kaolin Minerals Business

November 18, 2021
No Comments

KaMin LLC, a global performance minerals company owned by IMin Partners, and BASF announced that they have entered into a definitive agreement in which KaMin will acquire the BASF kaolin minerals business. 


Read More

Extender from Evonik

August 1, 2017
No Comments

Structurally modified, hydrophilic AEROSIL® improves the antifouling properties and product life of antifouling coatings.


Read More

BASF Receives Supplier Award From Behr Paint

August 30, 2015
No Comments

BASF in conjunction with HORN, its extender distributor in the western region of the United States, received the 2014 Supplier Excellence award from Behr Paint.


Read More

Functional Fillers for Matting and Performance Enhancements

in Waterborne, UV-Curable Coatings
Kevin Rink
June 1, 2015
No Comments

Ceramic microspheres may offer formulators alternatives in waterborne UV-curable coatings to serve as both a matting agent and functional performance filler.


Read More

Extender

Huber Engineered Materials
June 28, 2014
No Comments

Hydral® Coat 2 Ultrafine Alumina Trihydrate (ATH) is an extender developed for coil coatings.


Read More

Price Increase for IMERYS Carbonates North America

October 12, 2013
No Comments

Imerys Carbonates North America announced price increases for all calcium carbonate products


Read More

Huber Increases Price of Industrial Ground Calcium Carbonate

October 12, 2013
No Comments

Huber Engineered Materials, a division of J.M. Huber Corp., announced a price increase for its industrial calcium carbonate products.


Read More

Excalibar Minerals To Expand Corpus Christi Operations

September 8, 2013
One Comment

Excalibar Minerals LLC, a wholly owned subsidiary of Newpark Resources Inc., announced plans to add a new, fully automated 66‐inch Raymond Roller Mill to its grinding facility in Corpus Christi, TX.


Read More
Previous 1 2 Next
Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

industry news

Dozens Treated After Toledo Chemical Release

Mergers and aquisitions

Evonik Holds Off on BASF Takeover Talks

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

November 11, 2026

ChinaCoat

CHINACOAT2026 returns to Guangzhou this year. Welcome to exhibit, visit and join the annual industry gathering!

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing