Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » UV absorbers

Articles Tagged with ''UV absorbers''

a handshake over a horizon with individuals superimposed over the hands

SONGWON Enters Exclusive Partnership with KRAHN Italia

July 5, 2023
No Comments

Under the partnership agreement, KRAHN Italia becomes the exclusive distributor for SONGWON's BU Coatings range of SONGNOX® CS anti-oxidants, UV absorbers, and HALS products in Italy as of July 1, 2023. 


Read More
abstract design for European Coatings Show

Laser-Focused on Sustainability

Kristin Johansson
May 7, 2023
2 Comments

Sustainability dominated every conversation at the 2023 European Coatings Show. Learn about some of the innovative technologies that were introduced to help the industry formulate, manufacture, and apply the coatings of tomorrow.


Read More
Market-Reports (1)

SONGWON Reports 2022 Financial Results

March 6, 2023
No Comments

The group reported a strong first six months before overall demand began weakening in the third quarter as product availability grew and customers’ destocking activities increased in response to declining raw material costs.


Read More

SONGWON and SABO Extend Partnership

July 12, 2021
No Comments
Songwon Industrial Co. Ltd. recently announced that the worldwide exclusive distributor agreement (non-exclusive for Europe) with SABO S.p.A. for the SABOSTAB® HALS portfolio, which includes hindered amine light stabilizers and oxanilide UV absorbers, has been extended.
Read More
pci0620-Songwon-1044697294-900.jpg

Water-Miscible Stabilizers for Wood Coatings: A Synergistic Approach

Rosanna Telesca
July 16, 2020
One Comment
The new water-based additives and stabilization packages are designed to combine the efficiency of conventional products with the benefits of water miscibility and low to zero volatile organic compound (VOC) generation, as well as easy dosing and handling.
Read More
pci0819-FP-181132871-900.jpg

UV-Vis-Resistant Acrylic Latexes for Wood Coating Applications

by Encapsulation of Inorganic NPs Using Mini-Emulsion Polymerization
Gabrielle Boivin Anna M. Ritcey Véronic Landry
September 9, 2019
No Comments
In this work, mini-emulsion polymerization was used to prepare formulations containing various sizes of ZnO nanoparticles in order to increase photostabilization of exterior clear coatings for wood.
Read More

SONGWON and Omya Announce Distribution Partnership

April 6, 2018
No Comments
Omya announced a new distribution agreement with SONGWON Industrial Group for the United States and Canada.
Read More

Ultraviolet Absorbers from Songwon

April 1, 2018
No Comments

SONGSORB CS 400 is a liquid hydroxyphenyl triazine UV absorber with very high thermal stability and outstanding resistance in coatings exposed to high bake cycles or extreme external conditions.


Read More
basf

Waterborne UVA/HALS Blend

for High-Performance Clear and Pigmented Coatings
March 1, 2015
3 Comments

A novel water-dispersible blend combining a high-performance UV absorber with a non-reacting HALS was designed to fulfill the requirements for long-term weather resistance in exterior deco, decking and joinery markets.


Read More

Additive

CLARIANT
March 1, 2013
No Comments
The first high-loaded, water-based dispersion of a triazine-class UV absorber, Hostavin 3330 disp XP offers significant UV light protection for waterborne systems.
Read More
Previous 1 2 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Breaking News

Evonik Rejected €10.3 Billion BASF Offer, Reuters Reports

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing