Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » Weekly Web Articles

Weekly Web Articles
Weekly Web Articles RSS Feed RSS

20221122-covestro-at-trustech-2022-pic.jpg

Pushing Boundaries in ID Document Innovations

February 9, 2023
No Comments

Covestro offers a comprehensive specialty films portfolio for producing highly secure ID documents, such as passports and e-ID cards. 


Read More
Lead Image.JPG

Selective Brush Plating: a Flexible, Automated Solution to Plating Challenges

SIFCO Applied Surface Concepts (SIFCO ASC)
February 2, 2023
No Comments

Innovation continues at a great pace in the area of plating automation. The latest development comes in the form of a fully portable automated electroplating system, able to be moved directly to a specific component for in situ plating. 



Read More
GettyImages-530583272.jpg

Hygienic Coatings Prevent the Spread of Bacteria Safely

Teknos
January 27, 2023
No Comments

Teknos developed hygienic coatings for use in public spaces where there is a lot of movement, and infections spread easily. Study results confirm that these coatings are both safe and effective.


Read More
Lead Image.jpeg

Industrial Safety: Preventing Slips and Falls Virtually Everywhere

Del Williams
January 20, 2023
2 Comments

A new category of durable, high-tech, all-epoxy coating is dramatically increasing traction and improving safety in a wide range of slip and fall prone areas such as production floors, warehouse space, loading docks, platforms, ramps, and more.



Read More
GettyImages-1214122572.jpg

Coatings are a Game Changer in Pest Control

Tony Gonzales
January 12, 2023
3 Comments

Pest control coatings are truly innovative. By targeting a crawling pest’s inability to climb a smooth surface, a physical barrier around a home can be created with a coating.



Read More
Lead Image.png

Waterborne Conductive Primer/Adhesion Promoter with Graphene Nanotubes

Shows Sustainable Approach in Auto Industry
OCSiAl
January 9, 2023
One Comment

The new light-grey primer provides stable surface resistivity, strongly improving the adhesion between primer and base/clear coat on TPO car parts. A colloidal suspension of powder in water can be sprayed with standard liquid equipment devices while performing like a powder coating. 


Read More
Singulus_colored_coatings.jpg

Sustainably and Economically Coating 3D Components with Titanium

Singulus Technologies
January 1, 2023
No Comments

Singulus Technologies has developed a new layer system with titanium for sustainable coatings with the DECOLINE II production line. The innovative coating process reduces the necessary production steps and is, therefore, significantly more economical. 


Read More
Lead Image.png

Next-Generation Powder Coatings Shift from Pre- to Post-Consumer Recycled Plastic Resins

Sherwin Williams
December 23, 2022
No Comments

A line of powder coatings from Sherwin-Williams are now formulated with trailblazing polyester resins comprised of 25 percent post-consumer recycled plastic (rPET).


Read More
Lead Image.jpg

“Pigging” Technology Reduces Carbon Footprint

HPS Hygienic Pigging Systems
December 15, 2022
No Comments

Manufacturers of paints and coatings can now reduce their carbon footprint, every day, by using a liquid product recovery (often called 'pigging') technology, according to a new report from independent sustainability and energy consultancy Carbon-Zero.


Read More
Lead Image.jpg

How Are Electric Vehicle Battery Coatings Improving the Auto Industry?

Emily Newton
December 9, 2022
No Comments

Internal combustion engines (ICEs) are falling out of fashion to make way for battery electric vehicles (BEVs). Many components, including battery packs and power conversion parts, should have coatings to increase the car’s longevity, and to help with the issues BEV batteries bring. Creative solutions are coming out of the industry to help maintain BEVs for longer. 


Read More
Previous 1 2 … 14 15 16 17 18 19 20 21 22 … 108 109 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Breaking News

Evonik Rejected €10.3 Billion BASF Offer, Reuters Reports

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing