Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » Finished Products

Finished Products
Finished Products RSS Feed RSS

Interior Paint and Primer

April 30, 2016
No Comments

BEHR MARQUEE Interior’s one-coat coverage guarantee is expanding from 372 handpicked colors to more than 1,000 high-performance hues.


Read More
MotionCoat

UV Coating System

April 27, 2016
No Comments

ACTEGA North America has added MotionCoat™ to its specialty coatings portfolio.


Read More

Blast Primer

April 27, 2016
No Comments

The newly released Pro-Cryl 7000 by Sherwin-Williams is a water-based pre-fabrication blast primer that provides temporary protection for steel surfaces prepared by abrasive blast cleaning.


Read More
Jotachar 1709

Intumescent Coating

March 28, 2016
No Comments

Jotachar 1709 is a mesh-free epoxy passive fire-protection coating for the hydrocarbon processing and energy industries.


Read More

Powder Coatings

March 28, 2016
No Comments

The Diamond Collection features 15 classic black, white and clear-coat powders with varying degrees of shimmer and sparkle.


Read More

Urethane Primers

March 28, 2016
No Comments

SPECTRACRON® SPU conductive and non-conductive urethane primers are the first products of their kind to be engineered for application over multiple plastic substrates, such as METTON® LMR (liquid molding resin) and sheet-molded composite (SMC) plastics.


Read More

Architectural Coating

March 28, 2016
No Comments

INFINITY® is a complete, one-coat paint and primer in one with exceptional hiding power and coverage.


Read More

Waterborne Marking Paint

March 24, 2016
No Comments

BioStripe® is a soy-based marking paint ideal for any zone marking or traffic marking application.


Read More
WoodCoatings-123946969.jpg

Wood Coatings

March 24, 2016
No Comments

Developed to deliver on the staining needs of the professional, the new Flood Pro Series line combines popular existing formulas with several new and improved formulas to provide highly durable products with easy application.


Read More

Peel-Off Coating

February 29, 2016
No Comments

MCI® Peel-off Coating is a corrosion-inhibiting, modified water-based acrylic peelable coating powered by Migrating Corrosion Inhibitors (MCI) technology.


Read More
Previous 1 2 … 46 47 48 49 50 51 52 53 54 … 72 73 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Evonik Logo

Evonik to Close Two German Sites

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Breaking News

Evonik Rejected €10.3 Billion BASF Offer, Reuters Reports

Webinar custom content box

Events

October 8, 2026

AI-Powered Reformulation: Finding PFAS-Free, Lower-VOC Formulations Faster

In this webinar, we will use case studies from industry to illustrate how AI can be used to identify PFAS-free formulations and select surfactant blends for water-based products.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing