Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » FT Archives

FT Archives
FT Archives RSS Feed RSS

EQUIPMENT: Dry Ice Blaster

January 1, 2007
No Comments
KÄRCHER INDUSTRIAL PRODUCTS: The new IB 15/80 dry ice blaster is designed to provide an effective and mess-free method for in-place cleaning that eliminates the need to disassemble machinery before it is cleaned.
Read More

EQUIPMENT: Energy Efficient Process Chiller

January 1, 2007
No Comments
DOMNICK HUNTER: The Hyperchill process chiller technology is designed to provide a high refrigeration yield for low electrical consumption in finishing applications such as e-coat and thermal spray.
Read More

MATERIALS: Textured Release Coating

January 1, 2007
No Comments
KECO COATINGS AND RIVERS METAL PRODUCTS: KECO Coatings, in conjunction with Rivers Metal Products, has developed the KECO 600 Tex/Release™ Coating™, a textured composite coating that combines the toughness of tungsten carbide and the release properties of Teflon®
Read More

MATERIALS: FDA-Approved Coatings

January 1, 2007
No Comments
VICTREX PLC: Key grades of the recently introduced VICOTET Coatings and the high-temperature VICTREX® PEEK-HT polymer now comply with the compositional requirements of regulation 21 CFR 175.300 for resinous and polymeric coatings of the U.S. Food and Drug Administration (FDA).
Read More

MATERIALS: Fast Masking System

January 1, 2007
No Comments
DYMAX CORP.: SpeedMask® UV-curable masking resins are a new easy-on, fast-off masking system that is designed to replace cumbersome and costly, labor-intensive, multi-step processes that use adhesive tapes or solvent-based lacquers during dry or wet chemical surface treatment processing.
Read More

Ask Joe Powder

January 1, 2007
No Comments
Dear Joe,
In polyester/TGIC systems, the Tg is sensitive. Every weight percentage of TGIC reduces the Tg by approximately 1.5 to 2ºC. Why does TGIC reduce the Tg of the coatings
Read More

People

January 1, 2007
No Comments
Aleta Richards
Vice President, Coatings Marketing Unit, Bayer MaterialScience
Read More

Finishing Viewpoint

January 1, 2007
No Comments
Ring out the Old, Ring in the New
Read More

Don't Throw Away Your Filters

Kevin Biller
December 1, 2006
No Comments
A filter cleaning service is allowing finishers to improve their operating costs while reducing their environmental impact.
Read More

Ask Joe Powder

December 1, 2006
No Comments
Hello Joe,
We currently use 1K paint on OEM parts and are planning to build a mini-line to paint powder on class A parts
Read More
Previous 1 2 … 116 117 118 119 120 121 122 123 124 … 231 232 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing