Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » FT Archives

FT Archives
FT Archives RSS Feed RSS

International Paint Provides PSPC Advice to Chinese Shipyards - Posted 6/6/07

June 6, 2007
No Comments
Akzo Nobel’s International Paint business has teamed up with Lloyd’s Register to offer shipyards in China step-by-step advice on how to prepare to meet the requirements of the new Performance Standard for Protective Coatings (PSPC).
Read More

Carboline Acquires Finnaren & Haley Assets - Posted 6/6/07

June 6, 2007
No Comments
Carboline Co., a wholly owned subsidiary of RPM International Inc. and a manufacturer of high performance coatings, lining systems and fireproofing, has acquired the Marine and Industrial Assets of Finnaren & Haley, headquartered in Conshohocken, PA, a national supplier of marine, industrial and architectural products.
Read More

3M Acquires Diamond Productions - Posted 6/6/07

June 6, 2007
No Comments
3M has acquired Diamond Productions Inc., a manufacturer of superabrasive diamond and CBN (cubic boron nitride) wheels and tools for dimensioning and finishing hard-to-grind materials in metalworking, woodworking and stone fabrication markets. Terms of the transaction were not disclosed.
Read More

Vulcanium Staff Members Achieve CEF Certification - Posted 6/6/07

June 6, 2007
No Comments
Every member of Vulcanium Corp.’s engineering and sales office has passed the Certified Electroplater-Finisher (CEF) exam. “This commitment to quality assures all anodizing and plating customers that Vulcanium offers the best trained design and problem solving staff in the metal finishing industry,” the company said in a statement.
Read More

MATERIALS: Bright Acid Zinc Plating Process - Posted 6/6/07

June 6, 2007
No Comments
ENTHOBRITE® CLZ-970 bright acid zinc plating process has been introduced by Enthone Inc., a business of Cookson Electronics. The process is designed to provide the high productivity of a water-soluble process, while maintaining superior distribution and deposit properties at any chloride level.
Read More

MATERIALS: Water-Based UV Gloss Coatings - Posted 6/6/07

June 6, 2007
No Comments
ICA Group has developed a new line of water-based UV gloss coatings for use as final topcoats on wood furniture and accessories. These new polishable, monocomponent UV coatings are available in both transparent (UVA900) and pigmented (UVA901) versions.
Read More

EQUIPMENT: Updated Dry Disc Finisher - Posted 6/6/07

June 6, 2007
No Comments
Nova Finishing Systems Inc. has introduced a revised Nova-Hutson DF-14 dry disc finisher. The unit has a closed-loop dust collection system with a cover/lid and vacuum provisions for cleaner dry media operations and maintenance.
Read More

EQUIPMENT: Airblast Etching System for Pressure Plate Manufacturing - Posted 6/6/07

June 6, 2007
No Comments
Wheelabrator recently designed and manufactured an automated airblast etching system for pressure plate manufacturing. The process required a suitable “etched” finish to be imparted on one or both sides prior to introducing the pressure plate to a bonding process.
Read More

LITERATURE: Powder Wetting Brochure - Posted 6/6/07

June 6, 2007
No Comments
Powder Technologies, Inc. is offering a new four-color, 20-page brochure on Ystral mixing/dispersing and powder wetting technologies for a range of applications.
Read More

Registration Deadline Approaches for AESF Foundation SUR/FIN Courses - Posted 6/6/07

June 6, 2007
No Comments
The AESF Foundation SUR/FIN courses will be held at the Cleveland Convention Center, Cleveland, OH, during SUR/FIN 2007.
Read More
Previous 1 2 … 85 86 87 88 89 90 91 92 93 … 231 232 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing