Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » Paint & Coatings Industry Top Stories

Paint & Coatings Industry Top Stories
Paint & Coatings Industry Top Stories RSS Feed RSS

chemistry vials in a laboratory

The Future of Chemical Recycling for Latex Binders

Transforming Sustainability
Giona Kilcher
September 13, 2024
One Comment

In an interview with PCI, Giona Kilcher, Global Business Director, CASE, at Trinseo, delves into how chemical recycling, traditionally associated with plastics, is now being harnessed to make latex binders for coatings more environmentally friendly.


Read More
sun rising over field of crops

Development of More-Sustainable Water-Based DTM Coatings, Part II

Soy-Alkyd Dispersion Paints
Debora L. Hense-Hric Kris Weigal
September 13, 2024
One Comment

The objective of this collaboration was to showcase the performance of sustainable, soy-based coating materials in real-world formulations, comparing them to benchmarks derived from petroleum-based counterparts. Part II of this series focuses on soy-alkyd dispersion paint. 


Read More
Jotun-primax_top-banner.jpg

A Revolution in Anti-Corrosives

Jotun
September 13, 2024
One Comment

With the launch of the industry’s first and only CX-rated anti-corrosive powder coating solution, industries now have access to proven technologies to protect critical equipment operating in the most challenging environments.


Read More
graphic representing the carbon footprint

Citrate Esters as Coalescents for Acrylic Dispersions

Elvin J. Servellon
September 11, 2024
One Comment

Bio-degradable citrate esters have excellent toxicological and eco-toxicological profiles, and provide good versatility and compatibility with numerous polymers. Read how they compare to standard coalescing agents.


Read More
door entryway into a house

An Easy Additive Approach for Replacing Fluorocarbon Surfactants

in Water-Based Paints for Hot Block Resistance
Lichang Zhou Brian Vest Linda Adamson
September 11, 2024
One Comment

One of the key performance properties formulators use fluorocarbon surfactants for is early hot block resistance. To address this need in architectural coatings, a study of alternative technologies was conducted and revealed that modifying a specific phosphate ester could provide a straightforward solution.


Read More
Tiny sample paint cans during house renovation, process of choosing paint for the walls, different green colors, color charts on background

Examining the Efficiency of TiO2 in Matt Paints

and Methods of Obtaining Optimal Dry Opacity Without Sacrificing Wet Hide
Paul F. Dietz
September 11, 2024
One Comment

In an attempt to improve the quality and performance of a matt paint without detriment to wet hide, a TiO2/PCC composite pigment with optimally spaced TiO2 can increase the scatter per unit TiO2, as well as the dry opactiy. 


Read More
1-InnovationInsights.png

The Intersection of AI and Materials Research

Victoria Scarborough Ph.D.
September 9, 2024
2 Comments

AI and machine learning inspire the discovery/design of new materials and the processes to manufacture them. Autonomous R&D pushes the envelope for building predictive models and platforms that drive high-throughput innovation. How did we get here so fast, and where will this global megatrend take us? 


Read More
Web-GettyImages-1304944260-1170x658.jpg

Graphene as a Chemical Additive

Increasing Durability in Architectonic Waterborne Latex Paints
Xavier Raby Rafael Dias da Silva
September 9, 2024
2 Comments

The use of graphene as a corrosion inhibitor in industrial coatings has been widely reported, but its assets for waterborne latex resin coatings are less known. Learn how graphene boosts the performance of asphalt and architectural coatings.



Read More
Architectural Coatings.jpg

The Architectural Coatings Market

Asia Pacific is the Largest and Fastest-Growing Market in Architectural Coatings
Atul Yadav Dhiraj Kumar
September 9, 2024
2 Comments

Significant growth of the construction industry, environmentally friendly characteristics, durability, and better aesthetic appearance are all driving architectural coatings consumption. Increasing investments in emerging markets and less-regulated regions provide growth opportunities for market players.



Read More
biochemical research and medical analysis abstract blue background

How to Get Started with AI—and Why You Need to Do That Now

Hannah Melia
September 7, 2024
4 Comments

Whether you are a specialty coatings company selling to an OEM, or a raw material company selling into a coatings company, you can use AI to deeply understand how your product impacts your customers’ performance so that you can recommend the correct product, charge based on value, and find a market niche with higher margins. Learn how to get started.


Read More
Previous 1 2 … 23 24 25 26 27 28 29 30 31 … 142 143 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Evonik Logo

Evonik to Close Two German Sites

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Breaking News

Evonik Rejected €10.3 Billion BASF Offer, Reuters Reports

Webinar custom content box

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing