Arkema announced that, effective Aug. 1, 2019, Brenntag North America Inc. will be the primary distributor in the United States for Arkema waterborne resins sold under the Encor®, Celocor®, Snap® and Neocar® trade names, and that effective Oct. 1, 2019, the company will be consolidating its distribution network in the southern half of the United States for CRAYVALLAC® Additives.
Ace Hardware Corp. and Benjamin Moore announced an expanded relationship that will make Benjamin Moore paints more widely available to DIY customers at locally owned Ace Hardware stores across the country.
Applied Graphene Materials (AGM) announced that Alltimes Coatings Ltd., a specialist in the supply and application of protective coatings for buildings, is launching its Advantage Graphene liquid coating roofing system, which offers significantly enhanced anti-corrosion performance delivered by the incorporation of AGM's graphene.
RadTech, the nonprofit trade association for ultraviolet and electron beam (UV+EB) technology, has joined the National Academy of Inventors as a Member Institution.
Elevance Renewable Sciences Inc. has certified two process residue streams, olefins and saturated heavy methyl esters, produced at its Gresik, Indonesia, bio-refinery as process residue under the International Sustainability and Carbon Certification EU system.
Greif, a global leader in industrial packaging products and services, has made a large-scale investment in a new blow-molding machine at its Casablanca plant in Morocco.