Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • China Issue Archive
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » News

News
News RSS Feed RSS

Photo of Brian Cheshire

Tnemec Announces New Sales Director of Water & Wastewater

July 13, 2022
No Comments

Tnemec recently welcomed Brian Cheshire as the new Sales Director of Water & Wastewater.


Read More
Photo of Ann Roever

Sheboygan Paint Names New VP of Sales

July 13, 2022
No Comments

Sheboygan Paint Co. has hired Ann Roever as Vice President of Sales.


Read More
Photo of car wheels with black coating

AkzoNobel to Buy Aluminum Wheel Liquid Coatings Business

July 12, 2022
No Comments

AkzoNobel has reached an agreement to acquire the wheel liquid coatings business of Lankwitzer Lackfabrik GmbH. 


Read More

California Enacts Packaging EPR Law

July 12, 2022
No Comments

California has become the fourth state in the nation to enact a packaging EPR law, which was signed into law by Governor Gavin Newsom. 


Read More

The ChemQuest Group Unveils New Website

July 12, 2022
No Comments

The ChemQuest Group has launched a new website at chemquest.com, which is tailored to better support communication of the company’s pillars of expertise. 


Read More
Illustration of the new Meter Mix Portfolio

METER MIX Restructures Product Portfolio

July 12, 2022
No Comments

METER MIX recently announced that it has restructured its product portfolio, allowing customers to choose between two different material categories: machines for processing liquids and machines for processing pastes.


Read More
Photo of Jonathan Stowell, Group Commercial Director Scott Bader, shaking hands with Satyen representative.

Scott Bader Acquires Satyen Polymers

July 12, 2022
No Comments

Scott Bader recently announced that India-based Scott Bader Pvt Ltd. (SBPL) has acquired the commercial business of Satyen Polymers Pvt Ltd (SPPL).


Read More

Stahl Announces Goal to Reduce Scope 3 Upstream Emissions

July 12, 2022
No Comments

Stahl is submitting a greenhouse gas (GHG) emissions reduction target that is aligned with the most recent guidance provided by the Science Based Targets initiative (SBTi). 


Read More

JNS-SmithChem Acquires Gulf Coast Chemical

July 11, 2022
No Comments

JNS-SmithChem LLC, a full-service distributor of specialty chemicals and raw materials, announced the acquisition of Gulf Coast Chemical (GCC), based in Tampa, Florida. 


Read More
Photo of solar panels on Teknos manufacturing facility

Teknos Installs Solar Panels at Site in Finland

July 11, 2022
No Comments

Finnish-based coating manufacturer Teknos has installed solar panels at its paint production factory in Rajamäki, Finland. 


Read More
Previous 1 2 … 317 318 319 320 321 322 323 324 325 … 921 922 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

Popular Stories

Breaking News

16 Taken to Hospitals After Incident at Massachusetts Coating Facility

Plaque sign on the outside of the United States Environmental Protection Agency

EPA Draft Finds Worker Risks From trans-1,2-Dichloroethylene

Solstice Logo

Solstice, Element Solutions Terminate $14.5B Deal

Webinar custom content box

Events

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing