Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Home » Keywords: » sustainable coatings solutions

Items Tagged with 'sustainable coatings solutions'

ARTICLES

image of the EcoVadis seal

Perstorp Receives Gold Medal for Sustainability From EcoVadis

October 27, 2023
No Comments

Since its founding in 2007, EcoVadis has grown to become the world’s largest and most trusted provider of business sustainability ratings, creating a global network of more than 100,000 rated companies.


Read More
Powdura ECO Hybrid Coatings

Sherwin-Williams Launches Powdura ECO Hybrid Product Line

July 31, 2020
No Comments
The General Industrial Coatings division of Sherwin-Williams has released Powdura® ECO Hybrid Coatings – the newest technology within the Powdura ECO powder coatings platform launched in April.
Read More
Automotive coatings providers

Axalta Scales Up Production of Advanced Waterborne Coating Systems in China

May 8, 2020
No Comments
Axalta has broken ground on the newest phase of its Jiading plant in Shanghai, which represents an important new investment in waterborne coatings by the company in China.
Read More

Chugoku Marine Paints to Supply Solvent-Free Epoxy for Water Ballast Tanks in South Korea

March 27, 2020
No Comments
Following many years of extensive prototype trials in field tests, Chugoku Marine Paints Ltd. is ready to launch a new solvent-free epoxy coating that can be applied to water ballast tanks with standard application equipment that meets new Korean regulations under the Atmospheric Environment Conservation Act for the management of VOCs.
Read More
recycling architectural coatings

PaintCare Celebrates 10 Years of Paint Recycling

November 22, 2019
No Comments
PaintCare is celebrating 10 years of providing consumer education and recycling opportunities for households, businesses and institutions that purchase paint, stain and varnish for use in their projects and operations.
Read More
powder coatings

Russian Building With Interpon Eco Coatings Receives Architzer A+ Award

November 7, 2019
No Comments
A futuristic "pyramid" in Moscow that uses low solar absorption powder coatings supplied by AkzoNobel has won a major architecture award.
Read More
sustainable coatings solutions

AkzoNobel Launches Recycled Paint

October 4, 2019
One Comment

AkzoNobel has launched recycled paint thanks to a partnership in the UK with resource management experts Veolia.


Read More
sustainable automotive refinish

BASF Awarded Prize for Sustainable Development

June 28, 2019
No Comments
BASF's Coatings division was awarded the Pierre Potier prize medal in the Environmentally Friendly Process category for its R-M® eSense automotive paint line.
Read More

Beckers Group Publishes 2018 Sustainability Report

June 21, 2019
No Comments
Global industrial coatings company Beckers Group has published its 2018 Sustainability Report, giving a comprehensive picture of the company's activities last year and showing the progress it has made.
Read More
sustainable coating solutions

Powder Coatings

June 14, 2019
No Comments
Powder coatings have always offered customers numerous environmental benefits - now they've become even more sustainable following the launch of a full range of Interpon Low-E products developed by AkzoNobel.
Read More
More Articles Tagged with 'sustainable coatings solutions'
Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

industry news

Dozens Treated After Toledo Chemical Release

Mergers and aquisitions

Evonik Holds Off on BASF Takeover Talks

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

November 19, 2026

Reformulating Paints with AI: Turn Change into a Competitive Advantage

Join industry leaders and experts for real case studies showing how AI helps R&D teams use existing paint formulation and test data to evaluate alternatives, predict trade-offs, and prioritize experiments.

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing