Chemline specially formulated wood coatings offer OEMs higher production levels and lower labor costs because they are fast cure and require a minimal staging/curing area. They provide a superior protective barrier for wood, even in the harshest environments, such as temperatures below -20° F. Unique in the industry, applied Chemline polyurea coatings resemble traditional vinyl or ABS plastic with a textured-style appearance that forms a slip-resistant and waterproof barrier for wooden surfaces.
Idea for virtually any wood surface, these coatings feature 100 percent solids (no VOCs), rapid-curing polyurea (5-10 second gel times), Class A fire-resistant formulation when required, and a coating hardness of 45-60 Shore D.