Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Company News

VersaFlex Inc. and Renner Coatings Sign Partnership Agreement for Brazil and Chile

January 2, 2017

CURTITIBA, Brazil - Renner Coatings and VersaFlex Inc. have signed a co-labeling agreement to provide VersaFlex's line of pure polyurea systems to the Brazilian and Chilean markets.

Under the agreement, Renner Coatings will have access to the full line of VersaFlex Inc.'s pure polyurea coatings, membranes, sealants, and repair materials and coatings marked under the RenFlex™ name. In addition, Renner Coatings will also provide training and qualification to applicators, specifiers and engineers in conjunction with Polyurea University, taught by Dudley Primeaux II.

"The agreement between VersaFlex and Renner Coatings is promising and meets the objectives of increasing our presence in South America," said Todd Gomez, International Sales Manager at VersaFlex Inc.

"We are excited to be working with Renner Coatings, the largest 100% Brazilian high-performance coatings company," said Fernando Costa, Sales Manager at VersaFlex South America. "This will allow us to offer our high-quality polyurea systems to Renner Coatings customers in markets previously unavailable."

 

KEYWORDS: Brazil coatings manufacturers

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Industrial Coatings
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Evonik Logo

Evonik to Close Two German Sites

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

Webinar custom content box

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Related Articles

  • Ashland Announces Partnership Agreement for Spain and Portugal

    See More
  • VersaFlex Inc. and Raven Lining Systems Merge

    See More
  • BASF Coatings Signs Global Preferred Partnership Agreement with INEOS Automotive.jpg

    BASF Coatings Signs Global Preferred Partnership Agreement with INEOS Automotive

    See More

Related Products

See More Products
  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

  • intelligent.jpg

    Intelligent Coatings for Corrosion Control 1st Edition

See More Products

Related Directories

  • Stonebridge Coatings Laboratory Inc.

    Stonebridge Coatings Laboratory, Inc., is an ISO 17025 accredited, independent testing lab serving the paint, coatings and related industries. Services include competitive benchmarking, testing, failure analysis, product development, custom paint manufacturing and more. Stonebridge assists in identifying customer needs, developing a plan to address them, implementing the work and communicating successful outcomes.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing