Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Industry News

Researchers Design Coating to Prevent Pipeline Clogging

April 23, 2017

CAMBRIDGE, MA - A new coating solution developed by a team at MIT could stop buildup of hydrate ices that slow or block oil and gas flow.

When the Deepwater Horizon oil rig suffered a catastrophic explosion and blowout on April 21, 2010, leading to the worst oil spill in the history of the petroleum industry, the well’s operators thought they would be able to block the leak within a few weeks. On May 9 they succeeded in lowering a 125-ton containment dome over the broken wellhead. If that measure had worked, it would have funneled the leaking oil into a pipe that carried it to a tanker ship above, thus preventing the ongoing leakage that made the spill so devastating. Why didn’t the containment work as expected?

The culprit was an icy mixture of frozen water and methane, called a methane clathrate. Because of the low temperatures and high pressure near the seafloor, the slushy mix built up inside the containment dome and blocked the outlet pipe, preventing it from redirecting the flow. If it hadn’t been for that methane clathrate, the containment might have worked, and four months of unabated leakage and widespread ecological devastation might have been prevented.

Now, a team of researchers at MIT has come up with a solution that might prevent such a disastrous outcome the next time such a leak occurs. It may also prevent blockages inside oil and gas pipelines that can lead to expensive shutdowns to clear a pipe, or worse, to pipeline rupture from a buildup of pressure.

The new method of preventing the icy buildup is described in a paper in the journal ACS Applied Materials and Interfaces, in a paper by Associate Professor of Mechanical Engineering Kripa Varanasi, postdoc Arindam Das, and recent graduates Taylor Farnham and Srinivas Bengaluru Subramanyam.

The key to the new system is coating the inside of the pipe with a layer of a material that promotes spreading of a water-barrier layer along the pipe’s inner surface. This barrier layer, the team found, can effectively prevent the adhesion of any ice particles or water droplets to the wall and thus thwart the buildup of clathrates that could slow or block the flow.

Unlike previous methods, such as heating of the pipe walls, depressurization, or using chemical additives, which can be expensive and potentially polluting, the new method is completely passive — that is, once in place it requires no further addition of energy or material. The coated surface attracts liquid hydrocarbons that are already present in the flowing petroleum, creating a thin surface layer that naturally repels water. This prevents the ices from ever attaching to the wall in the first place.

Existing prevention measures, known as flow assurance measures, “are expensive or environmentally unfriendly,” says Varanasi, and currently the use of those measures “runs into the hundreds of millions of dollars” every year. Without those measures, hydrates can build up so that they reduce the flow rate, which can reduce revenues, and if they create blockages then that “can lead to catastrophic failure,” Varanasi says. “It’s a major problem for the industry, for both safety and reliability.”

The problem could become even greater, says Das, the paper’s lead author, because methane hydrates themselves, which are abundant in many locations such as continental shelves, are seen as a huge new potential fuel source, if methods can be devised to extract them. “The reserves themselves substantially overshadow all known reserves [of oil and natural gas] on land and in deep water,” he says.

But such deposits would be even more vulnerable to freezing and plug formation than existing oil and gas wells. Preventing these icy buildups depends critically on stopping the very first particles of clathrate from adhering to the pipe: “Once they attach, they attract other particles” of clathrate, and the buildup takes off rapidly, says Farnham. “We wanted to see how we could minimize the initial adhesion on the pipe walls.”

The approach is similar to that being used in a company Varanasi established to commercialize earlier work from his lab, which creates coatings for containers that prevent the contents — anything from ketchup or honey to paint and agrochemicals — from sticking to the container walls. That system involves two steps: first creating a textured coating on the container walls, and then adding a lubricant that gets trapped by the texture and prevents contents from adhering.

The new pipeline system is similar to that, Varanasi explains, but in this case “we are using the liquid that’s in the environment itself,” rather than applying a lubricant to the surface. The key characteristic in clathrate formation is the presence of water, he says, so as long as the water can be kept away from the pipe wall, clathrate buildup can be stopped. And the liquid hydrocarbons present in the petroleum, as long as they cling to the wall thanks to a chemical affinity of the surface coating, can effectively keep that water away.

“If the oil [in the pipeline] is made to spread more readily on the surface, then it forms a barrier film between the water and the wall,” Varanasi says. In lab tests, which used a proxy chemical for the methane because the actual methane clathrates form under high-pressure conditions that are hard to reproduce in the lab, the system performed very effectively, the team says. “We didn’t see any hydrates adhering to the substrates,” Varanasi says.

The research was funded by the Italian energy company Eni S.p.A. through the MIT Energy Initiative.

 

KEYWORDS: Protective Coatings Research and Development

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coating Pigments
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

BASF Ends Evonik Takeover Pursuit

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • Anti-Viral Surface Coating to Prevent the Spread of COVID-19 Through Touch

    Anti-Viral Surface Coating to Prevent the Spread of COVID-19 Through Touch

    See More
  • Harvard Researchers Design Most Durable Anti-Fouling Material to Date

    See More
  • Experts Explore Use of Antimicrobial Coatings to Prevent Spread of Drug-Resistant Bacteria

    See More

Related Directories

  • Formulator Software LLC

    At Formulator Software, we understand the precision and complexity involved in perfecting formulations. Our software is designed specifically for chemists, lab technicians, researchers, and manufacturers, providing essential tools to streamline the entire formulation process. Formed in 2002, Formulator Software is trusted by thousands to manage their raw materials, formulations, batch tickets, QC, SDS, COA, costing and more!
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing