Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Finishing News

Steelscape Pre-Painted Metal with DURANAR GR Coating Protects Washington School

September 5, 2017

PITTSBURGH – PPG and Steelscape have partnered to provide pre-painted metal coil finished with DURANAR® GR (graffiti-resistant) clear coating by PPG for the Issaquah Middle School project in Issaquah, Washington. It is the first school in the country to use the new coating, which PPG formulated to help U.S. building owners combat a problem that costs an estimated $25 billion per year.

Located near Seattle, Issaquah Middle School features a brick facade accented with architectural metal wall panels by AEP Span. Steelscape pre-treated the panels, which are used throughout the campus, with Duranar GR clear coating.

Steve Crawford, Director of Capital Projects for Issaquah School District, said Duranar GR coating is a sound investment. “While graffiti is not a significant issue in our school district, the graffiti-resistant coating was selected as a low-cost protection system to reduce potential damage and maintenance costs,” he explained.

Scott Cooley, Vice President of Sales, Steelscape, said that applying Duranar GR clear coating on metal wall panels enables manufacturers to offer architects an exclusive combination of design versatility and graffiti control. “In addition to offering architects high-performing and beautifully designed metal wall products, our customers now can deliver an affordable solution that makes it easier for building owners to maintain and preserve their property.”

Believed to be the only graffiti-resistant coating system sold and tested by the same company, Duranar GR coating features a clear, graffiti-resistant barrier over a metal building panel’s pigmented color layer. If a panel with the coating is spray painted or otherwise marred, it can be cleaned by applying DURAPREP® PREP™ 400 graffiti remover by PPG. After the remover is on the stain for 10 to 60 seconds, it can be wiped with a clean cloth or scrubbed with a nylon brush. Most stains can be removed in 10 minutes or less

When applied onsite on metal panels protected by Duranar GR clear coating, Duraprep Prep 400 graffiti remover eradicates graffiti as well as paint overspray, pen and marker ink, lipstick, scuff marks, tape residue, bugs, tar, and many other substances that mar the appearance of buildings.

Steelscape offers the pre-treated Duranar GR clear coating as part of its DESIGN SOLUTIONS® portfolio of metal coil, which features unique prints and high-performance coatings. 

For more information about Duranar GR clear coating, visit www.ppgmetalcoatings.com.

 

KEYWORDS: graffiti-resistant coatings Paint and Coating Manufacturers

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coating Pigments
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

Popular Stories

Breaking News

16 Taken to Hospitals After Incident at Massachusetts Coating Facility

USA election voters in red and blue to represent democrats and republicans

The AkzoNobel-Axalta Vote is Over. What Will Regulators Ask Next?

Plaque sign on the outside of the United States Environmental Protection Agency

EPA Draft Finds Worker Risks From trans-1,2-Dichloroethylene

Webinar custom content box

Events

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Related Articles

  • Steelscape Offers Pre-Painted Steel With Graffiti-Resistant Coatings

    See More
  • Prepainted Metal with Graffiti-Resistant Coating Provides Industry-First Protection for School Building

    Prepainted Metal with Graffiti-Resistant Coating Provides Industry-First Protection for School Building

    See More
  • architectural coatings

    New York’s Iconic VIA 57 West Finished with DURANAR Coatings

    See More

Related Products

See More Products
  • coatings.jpg

    Advanced Coating Materials

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing