Momentive Expands Distribution Agreement with Safic-Alcan in Europe
WATERFORD, NY – Momentive Performance Materials Inc. (Momentive) has expanded its distribution agreement with Safic-Alcan to include Eastern Europe. Effective immediately, Safic-Alcan will serve as an authorized distributor of Momentive’s specialty fluids and boron nitrides for personal care applications and specialty fluids for industrial applications in Eastern and Western Europe, providing customers with sales, order fulfillment and technical support.
“This agreement is a natural extension of a successful relationship that brings together Safic-Alcan’s extensive experience in specialty products and diverse markets with Momentive’s innovative specialty fluids and boron nitride powders that offer performance and processing benefits,” said Richard Perrin, Momentive’s Senior Sales Director–Specialty Fluids.