Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Industrial Coatings

OEMs Opt to Eliminate In-House Lamination Operations

Unichem
October 1, 2018

For OEMs that apply laminate films to metal parts or apply coatings to  as decorative finishes, the in-house manufacturing process requires a significant investment in equipment, plant floor space and ongoing maintenance for what can be a very temperamental process.

Not only that, but failure to precisely control what can be a very temperamental process can lead to laminates that do no bond properly or wrinkle, leading to excessively high scrap rates and even product returns.

For this reason, OEMs are increasingly outsourcing the application of laminate films to experienced coil coaters who can provide several alternatives: steel, aluminum or other metals in coil or sheet form with pre-applied (dry) adhesive; or fully laminated product that eliminates in-house processing altogether.

The result for OEMs can be significant, both in terms of speeding production and reducing operational costs. However, when paired with the fact that experienced coil coaters can produce high quality laminated products, it becomes a win-win scenario.

“Many OEMs are not fully aware of the alternatives for outsourcing part of, or all, the lamination operation to coil coaters,” explains Dan Chin, President of Universal Chemicals & Coatings (Unichem), a company that specializes in custom adhesives and coatings used in coil processing. “This is often simply because they have ‘always done it the same way’ – in house – but they can get a high quality laminated product and eliminate the costs and headaches associated with the process.”

 

Laminates

The use of laminate applied to metal to fabricate parts or products is widespread throughout manufacturing. Decorative finishes provide the look of stainless steel, brushed copper and wood grains, as well as a variety of colors, imprints and a range gloss levels. Laminate films can also serve a functional purpose by providing scratch or chemical resistance.

Some of the more common applications including appliances (refrigerators and freezers, washing machines, dishwashers, microwaves, range or fume hoods), construction products (insulated wall panels, garage doors, roofing products) and the mobile and manufactured home markets (walls, door panels).

Applying laminates to metal requires multiple steps. First, the metal is prepared by chemically cleaning and pre-treating. A liquid adhesive or film laminate is then applied to the metal and cured in an oven. The laminate film is then bonded to the metal as the adhesive-coated metal exits the oven and the laminate is fed into nip rollers to join the laminate to the adhesive. The laminated metal is then cooled.

According to Chin, in each step of the process there can be challenges that can lead to poor bonding or delamination.

“All kinds of things can happen during a non-continuous laminating process,” says Chin. “You can have issues with bonding caused by the cleanliness of the metal, improper application of the adhesive or insufficient oven temperatures. There could also be misalignments of the laminate that cause wrinkles in the film.”

Chin says this can lead to extremely high scrap rates in excess of 20%. Worse than that, OEMs may experience product returns and negative reviews due to delamination that occurs on a delayed basis once the product is in the field.

“If there is an issue with the bonding of the laminate, it can manifest later when a product is already in the hands of the customer,” says Chin. “Normally there would be quality control testing in place to ensure that doesn’t happen, but it is still possible. By the time the OEM finds out, it can become quite costly.”

 

Outsourcing to Coil Coaters

According to Chin, one option for OEMs is to turn to experienced coil coaters who can pre-apply B-stage adhesive to virtually any metal substrate. The B-stage adhesive is designed to reactivate and cure within a specific temperature range to bond the laminate. This eliminates several steps and can lead to a higher quality laminate bond.

“From a quality standpoint, you are going to get excellent uniformity of the adhesive applied [by a coil coater] and it will be properly cured,” says Chin. “Then, basically all the OEM has to do is laminate the film to the metal.”

Another option is to eliminate the entire process completely. This eliminates the need for in-house labor, application equipment, curing ovens, and environmental emission control systems.

“Typically, the coil coater has a lot of experience running these types of products, so they can dial in the adhesive thickness and control the curing and laminating temperatures very closely to ensure the proper bond,” says Chin. “That is going to translate to higher quality laminated product.”

Coil coaters must also guarantee scrap rates below a certain level.

“There is no testing the OEM will need to do, other than spot checks for their own quality monitoring process. The coil coater takes care of all that,” says Chin.

Chin adds that laminated coil can also be easily cut to just about any size, ready for stamping, forming or other finishing operations. This can eliminate several additional in-house steps and simplifies the process of maintaining an inventory of laminated metals in different sizes.

 

Adhesion Challenges

Experienced coil coaters are also better equipped to handle difficult adhesion challenges, often with the help of adhesive formulators like Unichem that can deliver custom formulations and provide other advice about the lamination process.

“As an adhesive formulator, we can customize the adhesive to match more exactly what the OEM is trying to accomplish,” explains Chin. “There are times the adhesive company, which has a specific catalogue of products, doesn't have a solution that works for specific applications.”

One example is adhesives formulated to be more “forgiving” in terms of temperature curing ranges. This can help OEMs that have challenges with oven temperature or consistency across the width of the coil.

“By working with the OEM or coil coater and understanding the parameters, we can help to dial in a solution that is very specific and resolve problems they are having in the bonding process,” says Chin.

Popular laminate films like TPO (thermoplastic olefin) are also notoriously difficult to bond to metal. TPO can refer to materials such as polypropylene (PP), polyethylene (PE), block copolymer polypropylene (BCPP) and others.

Although there are standard adhesives used to laminate to TPO, Chin says Unichem has seen enough variances that they have developed several custom solutions specifically designed for that material.

“As we have been formulating for TPOs, we have learned there can be really specific requirements as to the performance criteria and type of testing required that we have had to modify the adhesive significantly in order to get it to work for all the parameters,” says Chin.

Electrolytic Tinplate is another good example of a substrate that can be difficult to bond laminates and achieve the desired adhesion.

“Tinplate surfaces are very heat sensitive. Cure temperatures and other processing steps need to stay below 410 °F, or within a 390 - 410 °F range, otherwise tin re-flow can occur,” says Chin. This means that adhesives also need to cure or bond at temperatures below this temperature.

 

Time to Make the Switch?

Chin says that a good time to consider the transition is for plants that are utilizing aging equipment that can be time-consuming and costly to maintain or when scrap rates or performance issues with in-house laminating are excessively high.

“If the (lamination) equipment is 10 or 15 years old, it can become more problematic and require increasingly more maintenance. Outsourcing the entire process to coil coaters might be a better alternative than upgrading the equipment, which could be a huge investment,” says Chin

“Certainly in a manufacturing facility, the process of laminating can become a production bottleneck,” says Chin. “Because depending on the temperatures and thickness of the metal substrate, you can only process it a certain speed.” In some cases, outsourcing lamination operations – particularly those that are proving difficult and time-intensive – can speed up overall production.

“OEMs no longer have to worry about that if they receive laminated product in the sizes needed. They can immediately move to forming and finishing steps and definitely speed up production significantly if the laminating bottleneck is eliminated,” adds Chin.

For more information, call (847) 931-1700 or visit www.unicheminc.com.

 

By Unichem

KEYWORDS: Coil Coatings

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Architectural Coatings
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

PCI 2026 Voices from the Top eBook cover

eBook | 2026 Voices from the Top

The 2026 PCI 25

2026 PCI 25: Top Paint and Coatings Companies

AkzoNobel, Nippon

Nippon Paint Returns With €7.5B Proposal for AkzoNobel Business

The PCI 25 Annual Revenue Rankings

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
PCI Coat It! Podcast

Related Articles

  • exposure to lead-based paint

    The Powder Coating Research Group Partners With The Global Alliance to Eliminate Lead Paint

    See More
  • IPPIC Supports UN Actions to Eliminate Lead Paint

    See More
  • Photo of Elkem employee in hard hat

    Elkem Project Aims to Eliminate Carbon Dioxide Emissions from Silicon Production

    See More

Related Products

See More Products
  • laser tech.jpg

    Laser Technology: Applications in Adhesion and Related Areas

See More Products

Related Directories

  • Pigging Solutions

    Safe and operator-friendly pigging systems and piggable valves to recover trapped product from transfer lines and eliminate line flushing.
  • Pigging Solutions

    Safe and operator-friendly pigging systems and piggable valves to recover trapped product from transfer lines and eliminate line flushing.
  • ABM Equipment

    ABM Equipment is a systems integrator with over 50 years' experience engineering, fabricating, integrating, and servicing equipment and systems. In the paint industry ABM specializes in storage, handling, screening, and sifting for dry ingredients, and mixing for wet and dry. ABM distributes for many OEMs, manufacturing many pieces in-house.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing