Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Finishing News

Tnemec Introduces Polymer Concretes

polymer concretes
November 22, 2019

KANSAS CITY, MO – Tnemec Co. Inc., a manufacturer of industrial and architectural protective coatings, has introduced three chemical-resistant polymer concretes for use on new or existing surfaces. The LavaCrete series of high-performance polymer concretes can be applied and returned to service the same or next day and can cure at temperatures down to 40 °F, according to Dan O’Toole, Director of Sales-Food, Beverage and Specialty Markets.

“LavaCrete products are all about speed of installation and chemical resistance,” O’Toole explained. “These products are ideal for repairing heavily deteriorated concrete surfaces found in facilities where acid drips are common, such as pickling and plating plants, and for casting trenches, sumps, pads or secondary containment structures.”

Specific LavaCrete polymer concrete products include:

  • Series 469 non-shrinking, high-performance epoxy-based polymer concrete for refurbishment in low-temperature conditions where advanced corrosion resistance is required;
  • Series 479 non-shrinking, premium-grade novolac epoxy-based polymer concrete for added chemical resistance and fast return to service in regular and low-temperature conditions; and
  • Series 489 premium-grade vinyl-ester-based polymer concrete for pump and pad rebuilds in areas of strong acid and caustics.

“Because of their quick cure times, these products are often used in food processing plants where return-to-service time is measured in hours,” O’Toole added. “LavaCrete is also an industry standard for vibration-dampening, corrosion-resistant grouting material under the baseplates of motors and pumps.”

LavaCrete polymer concretes provide three times the bond of normal concrete when applied over surfaces prepared in accordance with SSPC-SP13/NACE 6 Surface Preparation of Concrete and ICRI Technical Guidelines. LavaCrete resists thermal shock and shrinkage and can be installed up to 10 inches in a single pour.

“With LavaCrete, corrosion protection is provided throughout the entire pour, regardless of its thickness,” O’Toole added. “Once the polymer concrete is in place, no additional coatings are required and return to service is usually within hours.”

Tnemec acquired the LavaCrete brand of high-performance polymer concretes under an agreement with St. Louis-based ProPolymer Coatings. For more information on ProPolymer coatings, e-mail inquiries to propolymer@tnemec.com or contact your local Tnemec sales representative.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Sustainable
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
PCI news now promo ad

Related Articles

  • protective coatings

    Tnemec Introduces Three New Endura-Shield Polyurethane Coatings

    See More
  • Series21 Tnemec

    Tnemec Introduces Series 21 Epoxolin

    See More
  • Advanced Polymer Introduces New E-Brochure

    See More

Related Products

See More Products
  • polymer coatings.jpg

    Polymer Coatings: Technologies and Applications

  • polymer.jpg

    Polymer Nanocomposite Coatings

  • pci november

    PCI November 2019 Issue

See More Products

Related Directories

  • STI Polymer

    Acrylic and styrene acrylic binders for elastomeric, concrete, metal, and specialty coating applications.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing