CAMBRIDGE, MA — Lambient Technologies LLC, provider of precision measurement solutions for the curing of advanced polymer materials, will now provide cure-testing services. These services extend the benefits of dielectric cure monitoring to organizations that may only have an occasional need to gather data about material cure.
With Lambient Technologies’ cure testing services, companies working with thermoset resins or advanced composites such as carbon fiber prepreg will gain the data necessary to improve manufacturing throughput. With this data, companies can identify flaws or inconsistencies in raw materials obtained from outside suppliers. Curing behavior can vary from batch to batch or even within an individual roll of a material such as carbon fiber prepreg. With data provided by Lambient Technologies, companies can work with suppliers to improve the consistency of raw materials.