SPHERILEX® DP-0115

SPHERILEX® DP-0115 is a new precipitated silica matting agent for powder coatings that enables efficient and consistent matting and appearance. Its uniform particle distribution improves hardness and flexibility of your powder coatings for use in metal and automotive applications, as well as for use on temperature-sensitive substrates such as wood and plastic. In addition, SPHERILEX® DP-0115 can be post-added to your coating formulation to adjust gloss.