Advanced Plastic Recycling from INEOS Olefins & Polymers USA Receives ISCC PLUS Certification
LEAGUE CITY, TX — INEOS announced that its manufacturing sites in Texas and California have been awarded ISCC PLUS certification from ISCC (International Sustainability & Carbon Certification). This certification supports recent successful, commercial-scale trials of Advanced Recycling technology for the production of ethylene, propylene, high-density polyethylene (HDPE) and polypropylene (PP).
Advanced Recycling converts waste plastic, which was destined for a landfill, back into a liquid raw material for use again in next-generation plastic production. Also known as chemical recycling, this technology can be used for many types of plastic including mixed plastic waste streams that are normally difficult or impossible to process with traditional recycling.