    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Company News

Stahl Receives Gold Rating from EcoVadis

July 16, 2021

WAALWIJK, Netherlands – Stahl recently announced that it has achieved an EcoVadis Gold rating, placing it within the top 5% of companies assessed by EcoVadis. The award underlines Stahl’s commitment to ensuring transparency in the value chain and collaborating with partners to improve the sustainability of operations and products.

EcoVadis is a globally recognized evidence-based assessment platform that reviews the performance of an organization across areas key to meeting sustainability targets, including the environment, labor and human rights, ethics, and sustainable procurement impacts. The latest report from EcoVadis highlights Stahl’s positive performance across all these areas.

This year’s Gold rating builds on the Silver rating achieved in 2020. In the past year, together with partners from across the value chain, the company has further committed to improving its environmental and social performance, protecting the communities in which it operates, and shaping a better chemical industry. Stahl’s 2030 target is to maintain the EcoVadis Gold rating through continual improvement.

Michael Costello, Director of ESG, commented, “Our new EcoVadis rating is a great achievement – one delivered through the hard work and dedication of many Stahl colleagues across the world. Our EcoVadis Gold rating underlines our commitment to ensuring a better world for all our stakeholders, and highlights that we are a trusted partner when it comes to ESG.”

Learn more about Stahl at https://www.stahl.com/.

KEYWORDS: Polymers for coatings sustainability

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Harvesting a field of soybeans with a combine harvester

Evaluation of Soy-Derived Solvents as PCBTF Alternatives in Industrial Alkyd Coatings

Lincoln Memorial Pool Coating

Lawsuit Puts Reflecting Pool Coating Project in the Spotlight

ACS 2026

ACS Organizers Reflect on 2026 Event, Preview 2028 Changes

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • carbon black

    Birla Carbon Receives Fifth Consecutive Gold Rating from EcoVadis

    See More
  • Chromaflo ecovadis gold

    Chromaflo Technologies Receives Gold Status CSR Rating from EcoVadis in EMEA

    See More
  • Corbion Receives Gold Sustainability Rating from Ecovadis

    See More

Related Products

See More Products
  • Optimizing Social Media from a B2B Perspective

  • pci may 2020

    PCI May 2020 Issue

  • Handbook of Adhesives and Sealants, Volume 1

See More Products

Related Directories

  • Orion S.A.

    Orion manufactures specialty carbon blacks for paint, coatings, ink, toner, adhesives, polymers, batteries, tires and rubber goods. Our specialty carbon blacks tint, colorize, impart conductive properties to, and enhance the performance of paints and coatings. The company runs 15 production sites and four Applied Technology Centers worldwide.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing