Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Finishing News

Chemical Coaters Association International Finishing Education Foundation Awards Scholarships

CCAIFEF scholarships
The Wisconsin chapter scholarship recipients attended the chapter golf outing and received their awards. (Photo courtesy of Chemical Coaters Association International.)
September 7, 2021

LAKEWOOD RANCH, FL – The Chemical Coaters Association International Finishing Education Foundation (CCAIFEF) recently announced its 2021 scholarship recipients. Since 1992, CCAI has awarded scholarship money from the CCAI Matt Heuertz Scholarship Fund to students enrolled in programs that could lead to a career in coatings and finishing. The scholarships are being awarded through the CCAIFEF, a 501 (c)(3) tax-exempt charitable organization. The CCAIFEF Board of Directors, which determined this year’s scholarship winners, reviewed applications from qualified students.

CCAIFEF awarded a total of $17,500 in scholarships to 10 students. “This year, we received applications from 28 individuals representing 14 different academic institutions,” noted Sheila LaMothe, CCAIFEF’s Executive Director. “We are excited to follow the career paths of these students as they are the future of the finishing and coatings industry.”

In addition to cash awards sent to the student’s school account, each scholarship recipient receives a one-year student membership in CCAI, which allows them to gain exposure to the industry and benefit from the resources available through the association and its chapters.

Recipients of a 2021 Matt Heuertz Scholarship include:

  • Genna Andreae, University of Wisconsin - Platteville;
  • Scott Andreae, University of Wisconsin – Stout;
  • Caiden Atienza, University of Iowa;
  • Joseph Ekes, Iowa State University;
  • Katie Engle, University of Cincinnati;
  • Emma Filipkowski, University of Cincinnati;
  • Dray Gibson, University of Cincinnati;
  • Tyler Kleinsasser, South Dakota School of Mines & Technology;
  • Gladwin Bryan Labrague, Missouri University of Science & Technology; and
  • William Joseph Martin, University of Cincinnati.

In addition to the National awards, the Twin Cities, West Michigan and Wisconsin CCAI chapters awarded nearly $20,000 through their own scholarships for students in their regions. The Twin Cities chapter recipients include: Kay Borgerding, North Dakota State University; Tyler Kleinsasser, South Dakota School of Mines & Technology; Olivia McCabe, College of Saint Benedict; Connor Quinlan, University of St. Thomas; and Carissa Stalzer, Iowa State University. The three West Michigan chapter scholarship winners are Anna Bielecki, Michigan State University; Carsen Bovink, Grand Valley State University, and Chloe Westrate, Saint Mary’s College-Notre Dame. The Wisconsin chapter awarded Tyler Kleinsasser, South Dakota School of Mines & Technology, the James Wright Scholarship. Genna Andrea, University of Wisconsin-Platteville, received the David Wright Scholarship, and Aaron Kinney, University of Wisconsin - Platteville received the James Steffes Scholarship. Additional Wisconsin chapter scholarship funds were awarded to: Sophia Brooks, Howard University; Adam Degler, University of Wisconsin – Madison; Jacob Diker, University of Wisconsin – Milwaukee; Alexandria Garczynski, University of Wisconsin – Milwaukee; Casey Roeser, University of Wisconsin – Madison; Mary Schilling, University of Wisconsin – Madison; and Nolan Wagner, St. Norbert College.         

CCAIFEF accepts scholarship applications each year beginning in January. Applications can be submitted online at www.ccaiweb.com.  

KEYWORDS: Chemical Coaters Association International finishing industry

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Sustainable
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
PCI news now promo ad

Related Articles

  • CCAIFEF Logo

    Chemical Coaters Association International Finishing Education Foundation Awards Scholarships

    See More
  • CCAI Webinars

    The Chemical Coaters Association International Presents Webinar Series

    See More
  • CCAI Finishing Education Foundation Accepting 2021 Scholarship Applications

    See More

Related Products

See More Products
  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

  • fluorinated2e.jpg

    Fluorinated Coatings and Finishes Handbook, 2nd Edition

See More Products

Related Directories

  • McCullough & Associates Inc.

    Distributor of specialty chemicals in the SE and SW USA. Celebrating our 58th anniversary in 2026. Recipient of the NACD RD Excellence Award in 2017.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing