  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Beverly Spears to Receive the 2021 Samson-Adler Award

October 18, 2021

On Tuesday morning, Beverly (Bev) Spears will receive the 2021 Samson-Adler Award. Beverly began her career in the coatings industry in 1986 as a Purchasing Manager for Preservative Paint in Seattle, WA. After eight years of purchasing she ventured into outside sales with Priestly Oil & Chemical (Now Tarr LLC), and opened the Washington Distribution Center and warehouse in Auburn WA. Her sales career progressed into positions in specialty chemical and industrial chemical sales and distribution for various industries, with emphasis on paint and coatings. She held positions with Synergistic Performance Corporation, Seggott Inc., and eventually invested as a partner with Cordano Chemical Company. In 2005, Cordano Chemical Company sold to Dorsett & Jackson where she managed the OR, WA, BC and ID territory until she retired in 2020.

 

Bev is Past President of PNWSCT(1989-1999) and has continued to serve on the board at different capacities and committees supporting the Symposiums. Bev serves as the SLC for PNWSCT since the inception of this National Committee and has held the Chair position in the past. Bev served on the WCS Board of directors for six years and three shows, and resigned in 2020.

 

Bev received the WCS Outstanding Service Award in 2019. She has received several Certificates of Participation from the Federation of Societies over the years, including the very first Annual Meeting Program Committee, which planned the initial short courses and classes for what is now known as the American Coatings Show.

 

Bev received the Distinguished Industry Achievement Award from the NPCA 1992 for coordinating paint and sundries distribution for eight homes and participating in Seattle’s Christmas in April program.

 

Bev volunteered at the PSPCA Annual Charity Dinner Auction for 10+ years, and the group raised over 150,000 for a variety of worthy causes. Bev was Head Chef for the ever-popular “Assole dinner for 12” that sold for top dollar at the event. Currently the group holds an annual paint and coatings toy drive and Christmas luncheon for charitable organizations.

 

Bev currently volunteers for The City of Renton, serves on the Maplewood Water Co-op, and holds the position as President for the private community Water District.

 

Bev resides at her home on the Cedar River with her partner, Greg, of 24 years. Between them they have five children and lost Bev’s son Daniel to a heart condition in 2010. They have eight very active grandchildren and one great grandson that they follow around golf courses, baseball and lacrosse fields, and ice rinks throughout the U.S.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coating Equipment
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

The 2026 PCI 25

2026 PCI 25: Top Paint and Coatings Companies

PCI 2026 Voices from the Top eBook cover

eBook | 2026 Voices from the Top

AkzoNobel, Nippon

Nippon Paint Returns With €7.5B Proposal for AkzoNobel Business

The PCI 25 Annual Revenue Rankings

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
PCI Coat It! Podcast

Related Articles

  • Miller Paint Company’s Kevin O’Leary to Receive 2019 Samson-Adler Award

    See More
  • James Calkin to Receive 2018 Samson-Adler Award

    See More
  • Romer Johnson Receives 2015 WCS Samson-Adler Award

    See More

Related Products

See More Products
  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products

Related Directories

  • WAB US Corp.

    WAB-GROUP® is a leading specialist in wet grinding technology, three-dimensional mixing technology and flow chemistry. The DYNO-MILL® wet milling and TURBULA® homogenous mixing brands support the paints and coatings industry globally with 70 years of experience. WAB is synonymous with highest efficiency, optimal performance, energy savings and lowest waste.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing