Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
New Products

GDB International Celebrates 25 Years and Showcases Revamped Product Range

March 24, 2022

To celebrate its 25th year, in addition to acquiring a 5M+ gallon capacity plant in 2021 to further boost production capabilities and quality, GDB International Inc. is showcasing its revamped product range at the American Coatings Show (Booth 1882) featuring eco-friendly coatings and products made under its flagship brand, Evolve.

 

The company recently announced it has developed a state-of-the-art paint recycling R&D center in Mt. Vernon, IL. This new research center will focus on providing environmentally friendly solutions in various segments of paint and powder coatings, ranging from the post-consumer architectural coatings, off-spec/distressed water-based and solvent-based coatings, and powder coatings. This centralized research center for GDB will be headed by Dr. Sagar Gade. Dr. Gade is a graduate of Missouri Science & Technology, with a Ph.D. in Chemistry. Dr. Gade has extensive knowledge and experience in the field of polymers and coatings. A team of distinguished professors headed by Dr. Vijay Mannari, Ph.D., Director of the Coatings Research Institute at the Eastern Michigan University, will oversee the first of its kind paint recycling training program.

 

Masters and bachelor's degree students from the field of paint and polymer technology will get an opportunity to earn project internships to learn the various aspects of paint recycling with a focus on environmental sustainability. Furthermore, GDB will launch a 3-day seminar in the Fall of 2022 to educate, promote and develop training programs to further the cause of paint recycling in the United States.

 

Over the last quarter century, GDB has grown into a multinational conglomerate within the global paint industry that excels in providing sustainable solutions. GDB has over 2 mm sq. ft of paint recycling and distribution facilities in North America where the company’s dedicated and hardworking team of 300+ employees have recycled over 120+ million gallons (1.2 billion lbs) of architectural coatings. Since 1993, the team of highly skilled chemists and R&D professionals have been working tirelessly to develop environmentally friendly solutions for the waste/ scarp generated within the paint industry.

 

Keeping the environment as its foremost priority, GDB’s paint recycling process adheres to a zero-waste policy. The company’s mission is to provide a sustainable solution for off-spec material to suppliers, offer economical paint to low-income families, and reduce waste streams to benefit the environment, and its growth is propelled by its constant need to innovate. The GDB Way encompasses a complete paint supply chain and turns it into a sustainable cycle by absorbing surpluses and post-consumer paint, leading the paint industry towards zero waste.

 

Following years of meticulous research and development, seeking the most viable environmental solutions for paint-related waste recycling, GDB today can re-utilize both oil and latex paints as well as raw materials in the most sustainable manner.

 

The company’s universal ‘cradle-to-cradle’ approach is at the center of its zero-waste policy, which begins with paint manufacturers, warehouses and distribution centers, paint retailers, consumer purchase, leading to the post-consumer program that brings paint back to our recycling center, where it is given a new lease of life.

 

For additional details, visit www.gdbpaint.com. 

 

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

Evonik Logo

Evonik to Cut 3,200 Jobs, Exit Polyester Business

Mergers and Acquisitions

Two Major Chemical Companies Plan to Combine

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • TMI Celebrates 25 Years

    See More
  • Evonik Tego Chemie GmbH Celebrates 25 Years

    See More
  • Kemira Site Celebrates 25 Years Without a Lost-Time Accident

    See More

Related Products

See More Products
  • January 25, 2024

See More Products

Related Directories

  • GDB International Inc.

    We are primarily manufacturer of new paint & coatings. We also deal in raw materials.
  • Catalytic Products International

    Solving complex air pollution control challenges by combining world-class engineering with extensive application experience to deliver regenerative thermal oxidizers (RTOs), thermal oxidizers, catalytic oxidizers, and precious metal catalyst products. Other services include consulting, turnkey installations, permitting assistance, and maintenance service contracts. Catalytic Products International...Enabling Clean Production since 1969.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing