Europlasma Signs Preferred Partnership with SCS for Nanocoatings
Europlasma is partnering with Specialty Coating Systems (SCS), a conformal coating services and technologies company, to expand its coating portfolio to include PlasmaGuard™ coating services. With this partnership, Europlasma grows the availability of its halogen-free PlasmaGuard conformal coatings for electronics. Applied through a plasma-enhanced chemical vapor deposition process (PECVD), ultra-thin PlasmaGuard™ nanocoatings are environmentally friendly, halogen-free, and provide excellent splash-proof and waterproof barrier protection to a wide range of electronic components and devices.
“Europlasma has been developing, fine-tuning, and delivering plasma surface treatment and coating solutions, and the systems to apply these solutions, for over 30 years,” said Europlasma CEO Tim Beulens. “We are excited to launch PlasmaGuard™ for electronics, together with SCS. We are pleased to have found in SCS a global partner that will provide contract coating services for Europlasma PlasmaGuard™ coatings to customers to achieve the highest performance and protection for their electronic products, with the lowest environmental footprint.”