Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Paint and Coating Resins & PolymersIndustrial CoatingsSustainable

Industrial Paint and Coatings 101

Exploring Alkyd Resins

By Sheboygan Paint Company
Colorfully painted fence around a playground
Credit: annalovisa / iStock via Getty Images Plus
October 31, 2025

Alkyds are a type of synthetic resin commonly used in industrial coatings. They are favored for:

  • Versatility: They can be formulated for a wide range of applications, from protective coatings to decorative finishes.
  • Durability: Alkyd coatings are known for their resistance to wear, weather and chemical exposure.
  • Gloss and Color Retention: They typically provide a smooth, glossy finish that maintains color over time.
  • Ease of Application: Alkyd-based coatings can be applied using various methods, including spraying, brushing or rolling.
  • Cost-Effectiveness: Generally, alkyds are more affordable than some other resin types, making them a popular choice in industrial settings.

While they offer many benefits, alkyd coatings can also have some limitations, such as longer drying times compared to other formulations and potential yellowing over time. Although chemical resistance and gloss retention of alkyds are good, they cannot match that of alternative chemistries such as urethanes. Cost savings from using alkyds versus alternative coatings are significant, which makes alkyds very favorable for industrial use. The widespread use of alkyds in industries like transportation, marine and general manufacturing highlights their effectiveness in protective and aesthetic applications.

The Chemistry
Alkyd resins are classified as thermoplastic polyesters synthesized via polycondensation reaction with polyhydric alcohol, polybasic acids or anhydrides, and fatty acids or triglyceride oils. They cure by both physical drying, where the solvent evaporates, and chemical curing. The chemical process, termed “autoxidative cure,” occurs when oxygen from the atmosphere reacts with the double bonds in drying oils to form cross-linking through radical reactions that increase the stiffness of the film at normal temperatures.

Metal drier compounds, such as cobalt, manganese, zirconium and others, have traditionally been used throughout the coatings industry to enhance the cure speed of alkyd coatings. Our Sheboygan Paint Company labs are actively testing new drier products developed by our suppliers to replace cobalt, which would offer safer and more sustainable alternatives for the environment.

The “oil length,” or percentage of oil to resin in the coating formula, can be adjusted in alkyds to influence the properties of the final product. Here’s how:

  • Drying Time: Longer oil lengths (more oil) generally result in slower drying times, which can be beneficial for certain applications where workability is essential.
  • Film Properties: Oil length affects the hardness and flexibility of the dried film. Short-oil alkyds (less oil) tend to be harder and more rigid, while long-oil alkyds provide increased flexibility and toughness.
  • Gloss and Appearance: The oil length can influence the gloss level of the coating. Longer oil lengths typically yield a glossier finish, which can enhance aesthetic appeal.
  • Chemical Resistance: Variations in oil length can affect the coating’s resistance to chemicals and environmental factors, which can be critical in certain industrial applications.
  • Adhesion: The oil length can also influence how well the coating adheres to substrates, impacting durability and performance.
  • Application Properties: Oil length can affect viscosity, making it easier or more challenging to apply depending on the desired application method.

While the amount of oil used in an alkyd resin dictates performance characteristics, so does the type of oil used. Here are some of the common oils used in alkyd resin production:

  • Drying Oils: Oils that harden into a tough, solid film through the oxidation process. Drying oils consist of glycerol triesters of fatty acids and are characterized by high levels of polyunsaturated fatty acids. Key components for many coatings and some varnishes, drying oils are being replaced more and more frequently by various alkyd resins.
  • Tung Oil: Also known as China wood oil, tung oil is a drying oil that is obtained by pressing the seed from the nut of the tung tree. This type of oil has been used since around the year 400 BC and is typically used on various wood products. After curing, this oil produces a very hard and easily repaired finish. Tung oil is also popular since it resists water better than any other pure oil finish.
  • Linseed Oil: Linseed oil, also known as flaxseed oil, is obtained from the dried, ripened seeds of the flax plant via a pressing process. It is often combined with other oils, resins and solvents, and is typically used in varnishes for wood coatings. Throughout the years, linseed oil has also been used as a plasticizer and hardener in putty and in the manufacturing of linoleum. As with tung oil, the use of linseed oil has declined over the years due to the increased use of synthetic alkyd resins.

Other natural oils used in the production of alkyd resins include soybean oil, safflower oil, sunflower oil, tall oil, castor oil and palm oil. Each type of oil contributes different properties to the final product.

The Result

By carefully adjusting oil type and length, formulators can tailor alkyd resins to meet specific performance and application requirements. For more information, click here.

KEYWORDS: Alkyd Resins Curing Agents formulating tips oils and resins thermoplastic polyurethanes

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coatings Additives
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

BASF Ends Evonik Takeover Pursuit

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • paint and coating manufacturers in England

    Industrial Paint Supplies (Hull) Gets a New Home

    See More
  • Aubel Joins HERR Industrial's Paint Sales Team - Posted 3/28/07

    See More
  • Young man on a large stone in the middle of the sea looking through binoculars

    Advanced Technologies for the Global Paint & Coatings Market

    See More
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing