Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Company News

Songwon Releases Third-Quarter Financial Results

ta graph and chart on blue technology background
Credit: Rasi Bhadramani / iStock via Getty Images Plus
November 14, 2025

Songwon Industrial Group released its financial results for the third quarter of 2025. The Group reported consolidated sales of 258,616 million KRW in the quarter, a decline compared to sales in the same period of the previous year. The company recorded a gross profit margin of 13.6% and a net profit of 1,697 million KRW.

For the first nine months of 2025, consolidated sales totaled 799,777 million KRW, reflecting a slight decline from the same period in 2024. The Group recorded year-to-date net profit of 5,073 million KRW and a gross profit margin of 14.3%.

The company provided a detailed breakdown of its financial performance:

SONGWON Q3 ResultsCredit: SONGWON

The global chemical industry continued to experience volatility in the third quarter. Division Industrial Chemicals recorded quarterly sales of 187,517 million KRW compared to the prior year’s period and year-to-date sales of 586,669 million KRW. Division Performance Chemicals reported quarterly sales of 71,099 million KRW and year-to-date sales of 213,108 million KRW.

Division Industrial Chemicals faced ongoing weak market conditions, intense competition, high energy costs in Europe, and the effects of trade measures on Asian markets. Improved pricing, lower raw material costs, and favorable currency effects helped mitigate some of the impact. Polymer Stabilizers saw lower volumes due to weaker demand in the United States and the removal of Hindered Amine Light Stabilizers from the portfolio, though turnover and margins remained aligned with expectations. Fuel and Lubricant Additives maintained steady volumes with softening revenues shaped by raw material pricing and geopolitical factors. Coatings recorded lower volumes and revenues in the quarter due to weaker demand and persistent pricing pressure.

Division Performance Chemicals delivered solid performance despite ongoing challenges. BU Tin recorded lower volumes due to weaker demand in Japan and EMEA and continuing global logistics constraints, but revenues held firm. PVC defended market share in Korea and remained active in new opportunities, with strong development in EMEA. Solution Polyurethanes and Thermoplastic Polyurethanes performed in line with expectations due to strong overseas sales.

Songwon anticipates a challenging fourth quarter influenced by seasonal factors, subdued global demand, overcapacity, and year-end inventory reductions. Despite expectations of slightly lower volumes compared to 2024, improved pricing and cost efficiency are expected to support turnover and gross margin. Strategic initiatives, including a new greenfield One Pack Systems plant in Saudi Arabia, are positioned to support future growth and help the company respond to evolving customer needs.

The full third-quarter report is available at www.songwon.com/investors/reports-publications.

KEYWORDS: chemical companies quarterly reports

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Evonik Logo

Evonik to Cut 3,200 Jobs, Exit Polyester Business

Mergers and Acquisitions

Two Major Chemical Companies Plan to Combine

Axalta and AkzoNobel logos

AkzoNobel and Axalta Set Key August Date for Proposed Combination

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Market-Reports.jpg

    Brenntag Releases Third-Quarter Financial Results

    See More
  • Market-Reports.jpg

    Evonik Releases Third-Quarter 2023 Financial Results

    See More
  • Market-Reports.jpg

    AmCoat Releases Third-Quarter 2023 Financial Results

    See More

Related Products

See More Products
  • organic coatings.jpg

    Organic Coatings: Science and Technology, 4th Edition

  • Cold Spray Technology

  • nanostructuredthinfilms.jpg

    Nanostructured Thin Films and Coatings: Mechanical Properties

See More Products

Related Directories

  • Songwon International - Americas Inc.

    Polymer additives including antioxidants, acid scavengers, thioesters, UV absorbers and hindered amine light stabilizers (HALS).
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing