The Drais Advantis(r) Perl Mill offers fine grinding down to 20 nanometers for coatings and pigment dispersions. With residence
times measured in 3-5 seconds, the equipment can achieve tight particle size distributions. The low-volume chamber offers easy
cleaning and rapid color changes. The silicon carbide inner stator provides excellent cooling. For more information, contact
Draiswerke Inc., phone 201/847.0600; fax 201/847.0606; e-mail salesinfo@draiswerke-inc.com; visit
www.draiswerke-inc.com.