AGA Chemicals Inc., a subsidiary of Japan's Asahi Glass Company, has introduced Lumiflon LF-710F, a 100%-solid polymer for powder coatings. In addition to featuring all the benefits of Lumiflon's solvent-soluble fluoropolymers, which include superior corrosion resistance, UV resistance, solubility and appearance, Lumiflon LF-710F boasts a 90-98% application rate (vs. 70-80% in solvent grades) and compliancy with international VOC environmental standards. For more information, contact Telly Wong, Dentsu Communications, TWong@dentsucommunications.com.