Self-Initiating Resin Ashland Specialty Chemical FlexCureTM self-initiating resins utilize a proprietary, energy-curable acrylic resin chemistry. Unlike conventional UV-cured resin systems, this new class of molecules is "self-initiating." With exposure to typical commercial UV energy dosages, optimum cure can be achieved with little or no photoinitiator. Call 614/790.3446.