The aim of this article is to provide a simple introduction to rheology, highlighting its applicability to the coatings industry. Basic rheological terms are defined, methods for their measurement are discussed with reference to the capabilities of rotational rheometers, and their relevance is outlined. A series of industrial examples highlights the practical benefits of rheological studies.