Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Breaking News

Nanotechnology Helps Preserve Silver Artifacts and Art

October 31, 2010

COLLEGE PARK, MD - Scientists from the A. James Clark School of Engineering at the University of Maryland, College Park, have teamed up with conservators from the Walters Art Museum in Baltimore, MD, to develop and test a new, high-tech way to protect silver art objects and artifacts, using coatings that are mere nanometers thick.

The technique, called atomic layer deposition (ALD), will be used to create nanometer-thick, metal-oxide films that, when applied to an artifact, are both transparent and optimized to reduce the rate of silver corrosion. The films are created when an object is exposed to two or more gases that react with its surface.

“ALD gives us an exquisite level of control, literally at the atomic level," said Ray Phaneuf, a professor of materials science and engineering (MSE) working on the project. "It's an effective, low-cost strategy to reduce corrosion that preserves artifact appearance and composition while complying with the rigorous standards of art conservation practice.”

Eric Breitung, a scientist who runs E-squared Art Conservation Science, proposed the collaboration after conducting preliminary investigations into the use of ALD on silver at New York's Metropolitan Museum of Art.

"I approached members of the Clark School faculty because of their expertise and the university's extensive ALD facilities at the Maryland NanoCenter," he said. He added that the faculty members' previous collaborations with museums made them a good match for the Walters and its silver collection.

Walters Art Museum Conservation Scientist Glenn Gates explains the goals the new coating has to achieve.

"First, its appearance must be acceptable for display in a museum context. It has to be tough enough to endure transport and handling, but not so tough that it can't be removed. It needs to be completely removable so an object can be re-treated to meet future standards of conservation and aesthetics. And finally, it should not cause any harm to a piece, even if it breaks down."

Gates, who works with the Walters' world-class silver collection, is well acquainted with the battle against tarnish. He points out the project's figurative mascot, Antoine Louis Barye's 1865 "Walking Lion" sculpture, as exactly the sort of piece that could one day benefit from the new treatment. It has been cleaned and lacquered twice since 1949, but in both cases ultimately experienced deterioration problems with its coatings. It is currently unlacquered but must be kept in a special exhibition case to ward off tarnish.

"The 'Walking Lion' represents a complex shape that, being difficult to coat with traditional lacquer, might benefit from ALD protection," Gates said.

The team will test the new technique, first on small samples of fine and sterling silver, and then on objects from Gates' own collection, such as 19th century demitasse spoons and Morgan silver dollars. While the Walters does not expect any pieces from its collection to receive the experimental treatment during the course of the study, once it has been proven effective and safe, the “Walking Lion” would be a prime candidate for this procedure.

The three-year project is one of the first to be funded by the National Science Foundation's Chemistry and Materials Research at the Interface between Science and Art (SCIART) grant program, which supports projects in the field of cultural heritage science through the funding of collaborations among conservation experts in museums and scientists in academia. The SCIART program will be highlighted at the 2011 national meeting of the American Chemical Society, which has invited the team to present their work.

The project's other team members include the museum's Director of Conservation and Technical Research Terry Drayman-Weisser, a recognized metals expert, and, from the University of Maryland's Department of Materials Science and Engineering, Professor Gary Rubloff, Research Associate Laurent Henn-Lecordier, and Graduate Assistant Amy Marquardt, who brings to the project her previous experience working on bronze patinas with the Smithsonian's Museum Conservation Institute.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Industrial Coatings
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Breaking News

Evonik Rejected €10.3 Billion BASF Offer, Reuters Reports

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event
PCI news now promo ad

Related Articles

  • Nanometer-Thick Metal Oxide Coatings May Help Preserve Silver Artifacts and Art

    See More
  • Lux Research: Nanotechnology Helps Profits by Cutting Energy Costs

    See More
  • Nanotechnology Helps Profits by Cutting Energy Costs

    See More
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing