Cross-linker Helps
Weather Resistance
Primid QM-1260 hydroxyalkylamide cross-linker is a white crystalline solid with
a melting point of approximately 105°C. It is recommended for high-performance
weather-resistant polyester powder coatings. It has excellent gas oven stability
and can be used to reduce discoloration under critical curing conditions. The
cross-linker's high initial whiteness improves the quality of white polyester
powder coatings.
EMS-Chemie (North America)
800-690-3887
Resin for
Low-Temperature Cure
Fine-Clad M-8950 resin cures at temperatures as low as 250°F. Suitable for
exterior applications, it exhibits excellent weathering resistance in formulated
powder coatings. It remains free-flowing when stored at 40°C for up to 1 month,
reducing blocking problems. Applications include thermally sensitive substrates
such as wood and plastics. Coatings formulated with the resin have end-uses
including interior and exterior metal parts, automotive underhood parts, and
lawn and garden equipment.
Reichhold Inc.
800-431-1920