AdBloc is designed to help manufacturers of plastic automotive parts meet federal emission standards for HAPs while meeting or exceeding industry standards for adhesion and resistance to humidity and gasoline spills. According to the company, the adhesion promoter has been approved by two of the major automotive original equipment manufacturers (OEMs) and is already being used by an automotive parts supplier to one of the OEMs.