The F20-UVX thin-film measurement system from Filmetrics uses an expanded wavelength range of 200 to 1700 nm for increased thin-film analysis capabilities. This new system can measure the thickness of films from 30Å to 450 µm thick and optical constants of films from 500Å to 10 µm thick.