Notre Dame Researchers Develop Paint-On Solar Cells
SOUTH BEND, IN - Imagine if the next coat of paint you put on the outside of your home generates electricity from light — electricity that can be used to power the appliances and equipment on the inside.
A team of researchers at the University of Notre Dame has made a major advance toward this vision by creating an inexpensive “solar paint” that uses semiconducting nanoparticles to produce energy.