Atlas® Material Testing Technology Forms Alliance with SGS
LINSENGERICHT, Germany – Atlas Material Testing Technology, a leader in accelerated weathering instruments and weathering testing services, has entered into an alliance with SGS, a leading inspection, verification, testing and certification company, allowing for the expansion of the Atlas 25+ PV module durability test program.
Consisting of a comprehensive battery of accelerated tests, the original Atlas 25+ program integrated both laboratory and outdoor environmental exposures, targeting the long-term product "wear-out" period that can result in declining module performance or outright failure.