Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Nanotechnology in Coatings

How Butterfly Wings Can Inspire New High-Tech Surfaces

April 1, 2013

A South American butterfly flapped its wings, and caused a flurry of nanotechnology research to happen in Ohio. Researchers have taken a new look at butterfly wings and rice leaves, and learned things about their microscopic texture that could improve a variety of products.

For example, the researchers were able to clean up to 85 percent of dust off a coated plastic surface that mimicked the texture of a butterfly wing, compared to only 70 percent off a flat surface. In a recent issue of the journal Soft Matter, the Ohio State University engineers report that the textures enhance fluid flow and prevent surfaces from getting dirty – characteristics that could be mimicked in high-tech surfaces for aircraft and watercraft, pipelines, and medical equipment.

“Nature has evolved many surfaces that are self-cleaning or reduce drag,” said Bharat Bhushan, Ohio Eminent Scholar and Howard D. Winbigler Professor of mechanical engineering at Ohio State. “Reduced drag is desirable for industry, whether you’re trying to move a few drops of blood through a nano-channel or millions of gallons of crude oil through a pipeline. And self-cleaning surfaces would be useful for medical equipment – catheters, or anything that might harbor bacteria.”

Bhushan and doctoral student Gregory Bixler used an electron microscope and an optical profiler to study wings of the Giant Blue Morpho butterfly (Morpho didius) and leaves of the rice plant Oriza sativa. They cast plastic replicas of both microscopic textures, and compared their ability to repel dirt and water to replicas of fish scales, shark skin and plain flat surfaces.

Common to Central and South America, the Blue Morpho is an iconic butterfly, prized for its brilliant blue color and iridescence. Beyond its beauty, it has the ability to cast off dirt and water with a flutter of its wings. For a butterfly out in nature, staying clean is a critical issue, Bhushan explained.

“Their wings are so delicate that getting dirt or moisture on them makes it hard to fly,” he said. “Plus, males and females recognize each other by the color and patterns on their wings, and every species is unique. So they have to keep their wings bright and visible in order to reproduce.”

The electron microscope revealed that the Blue Morpho’s wings aren’t as smooth as they look to the naked eye. Instead, the surface texture resembles a clapboard roof with rows of overlapping shingles radiating out from the butterfly’s body, suggesting that water and dirt roll off the wings “like water off a roof,” Bhushan said.

The rice leaves provided a more surreal landscape under the microscope, with rows of micrometer- (millionths of a meter) sized grooves, each covered with even smaller, nanometer- (billionths of a meter) sized bumps – all angled to direct raindrops to the stem and down to the base of the plant. The leaf also had a slippery waxy coating, which keeps the water droplets flowing along.

The researchers wanted to test how butterfly wings and rice leaves might display some of the characteristics of other surfaces they’ve studied, such as shark skin, which is covered with slippery, microscopic grooves that cause water to flow smoothly around the shark. They also tested fish scales, and included non-textured flat surfaces for comparison.

After studying all the textures close up, the researchers made molds of them in silicone and cast plastic replicas. To emulate the waxy coating on the rice leaves and the slippery coating on shark skin (which in nature is actually mucous), they covered all the surfaces with a special coating consisting of nanoparticles.

In one test, they lined plastic pipes with the different coated textures and pushed water through them. The resulting water pressure drop in the pipe was an indication of fluid flow.

For a pipe about the size of a cocktail straw, a thin lining of shark skin texture coated with nanoparticles reduced water pressure drop by 29 percent compared to the non-coated surface. The coated rice leaf came in second, with 26 percent, and the butterfly wing came in third with around 15 percent.

Then they dusted the textures with silicon carbide powder – a common industrial powder that resembles natural dirt – and tested how easy the surfaces were to clean. They held the samples at a 45-degree angle and dripped water over them from a syringe for two minutes, so that about two tablespoons of water washed over them in total. Using software, they counted the number of silicon carbide particles on each texture before and after washing.

The shark skin came out the cleanest, with 98 percent of the particles washing off during the test. Next came the rice leaf, with 95 percent, and the butterfly wing with about 85 percent washing off. By comparison, only 70 percent washed off of the flat surface.

Bushan thinks that the rice leaf texture might be especially suited to helping fluid move more efficiently through pipes, such as channels in micro-devices or oil pipelines.

As to the Blue Morpho’s beautiful wings, their ability to keep the butterfly clean and dry suggests to him that the clapboard roof texture might suit medical equipment, where it could prevent the growth of bacteria.

 

This research was funded by the National Science Foundation

KEYWORDS: Coating Research & Development nanotechnology

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coatings Additives
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

A robotic hand points at a glowing compliance concept surrounded by various icons representing laws, regulations, governance, and standards in a digital workspace

Powder Coater’s $1.64M OSHA Case Follows Earlier Citations

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • Butterfly Wings Could Inspire New Hue-Changing Materials

    See More
  • New High-Tech Microcorrosion-Inhibiting Coating

    See More
  • Gema Unveils New High-Tech Headquarters.jpg

    Gema Unveils New High-Tech Headquarters

    See More

Related Products

See More Products
  • 9781845692650.jpg

    High-Performance Organic Coatings 1st Edition

  • pci may 2020

    PCI May 2020 Issue

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing