Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » PFAS-free

Articles Tagged with ''PFAS-free''

PCI-1123-WCS-micro-powders.jpg

Micro Powders to Showcase New Natural and PFAS-Free Additives at CTT Summit

July 29, 2024
No Comments

In addition to exhibiting at the event, Vice President, Richard Czarnecki will participate in the event's keynote panel discussion and discuss Navigating Materials of Concern in the Coatings Industry.


Read More
Additives.jpg

PFAS-Free Additives for Continuous Processes

June 17, 2024
No Comments

Two innovative PFAS-free product solutions that master many current challenges in the production of films, pipes, profiles, fibers and much more prevent melt fracture, reduce the viscosity of the melt, reduce die build-up, and allow faster material changes.



Read More
1-InnovationInsights.png

Challenges of Sustainability in a Climate-Conscious World

Victoria Scarborough Ph.D.
June 4, 2024
No Comments

Human stewardship of the Earth is undergoing a metamorphosis—and for very good reasons. The planet is getting hotter, and the situation is getting worse. How can the paint industry, whose products literally cover the Earth, re-engineer its products and processes toward a more sustainable future?



Read More
PCI1123-Siltech-1-1170.jpg

Where Silicone Materials Can Replace Perfluoroalkyl Substances

Dr. Bob Ruckle Dr. Tom-Seung Cheung Yanjun Luo
November 3, 2023
5 Comments

For those looking to replace PFAS in their coatings formulations, this article discusses some experiments and data that show how organosilicones compare to PFAS compounds in critical performance criteria such as low surface tension/surface energy, COF, water repellency, oil repellency, stain resistance, and chemical stability.


Read More
Sustainability and Bio-based

Clariant Releases PTFE-Free Texturing Agent for Powder Coatings

October 20, 2023
No Comments

The company said rising concerns about the impact of PFAS on human health and the environment have led to a growing demand for PTFE alternatives.


Read More
GettyImages-1170x878-1198385761.jpg

A Close Shave

New PFAS-Free Alternatives to PTFE Surface Lubricating Coatings for Razor Blades Could Mean Great Shaving and a Better
Qian He Eric Hanson Edward Hughes
August 7, 2023
One Comment

Lubricating coatings on razor blades are thin films that reduce friction between the blade and the skin during shaving and reduce the force required to cut hair. A new class of nanoscale surface treatments are very promising candidates for replacing PTFE on cutting edges, and can provide good cutting performance and durability, while reducing the potential risks to the environment and human health. 


Read More
Previous 1 2 3 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Breaking News

Evonik Rejected €10.3 Billion BASF Offer, Reuters Reports

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing